POM TARNOFORM® TARNOFORM200 GRUPA AZOTY POLAND
237
- Unit Price:US$ 2,818 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
impact performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Impact strength of simply supported beam without notch | ---- | ISO 179/1eU | 无断裂 |
-30°C | ISO 179/1eU | 200 kJ/m² | |
Impact strength of cantilever beam gap | ISO 180 | 8 kJ/m² |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Ball Pressure Test | H358/30 | ISO 2039-1 | 140 Mpa |
Tensile modulus | ISO 527-1-2 | 2600 Mpa | |
tensile strength | Yield | ISO 527-2/50 | 60 Mpa |
Tensile strain | YieldYield | ISO 527-2/50 | 14 % |
BreakBreak | ISO 527-2/50 | 50 % | |
Bending modulus | ISO 178 | 2400 Mpa | |
bending strength | ISO 178 | 60 Mpa |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Hot deformation temperature | 1.8 MPa,Unannealed | ISO 75-2/A | 105 °C |
Vicat softening temperature | ISO 306/B | 150 °C | |
Melting temperature | ISO 11357-3 | 167 °C | |
Linear coefficient of thermal expansion | MD:23~55℃ | ISO 11359-2 | 0.00011 1/℃ |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183 | 1.41 g/cm³ | |
melt mass-flow rate | 190℃,2.16kg1 | ISO 1133 | 2.5 g/10min |
Melt Volume Flow Rate (MVR) | 190℃,2.16 kg | ISO 1133 | 2.2 cm3/10min |
Shrinkage rate | MD:2.0 mm | ISO 294-4 | 2 % |
Water absorption rate | Saturation,23℃ | ISO 62 | 0.8 % |
Equilibrium,23℃,50% RH | ISO 62 | 0.2 % |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Surface resistivity | IEC 60093 | 100000000000000 ohms | |
Volume resistivity | IEC 60093 | 1000000000000000 ohms·cm | |
Dielectric strength | 2 mm2.00 mm | IEC 60243-1 | 25 KV/mm |
Dielectric constant | 1 Hz1 Hz | IEC 60250 | 3.8 |
Compared to the anti leakage trace index | Solution A | IEC 60112 | PLC 0 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
ISO TypeISO Type | ISO 1874 | POM-K. M-GNR. 01-02 |
flame retardant performance | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | 3.20 mm | UL 94 | HB |
Burning rate | FMVSS 302 | < 100 mm/min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.