PC PANLITE® MN-3600HS CM70206HS TEIJIN JAPAN
202
- Unit Price:US$ 3,763 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:20MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:heat-resisting|Flame retardant|Good impact resistance|Good liquidity|Halogen-free|Electrical field|Electronic field|Automotive sector
- Application Areas:Lighting applications
- Color:--
- Grade:Flame retardant grade
Technical Data Sheet
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D792 | 1.19 g/cm³ |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | 断裂 | ISO 527-2/5 | 50 Mpa |
elongation at yield | ISO 527-2/50 | 7 % | |
Heat Deflection Temperature | 0.45 MPa, 未退火 | ISO 75-2/B | 125 °C |
1.8 MPa, 未退火 | ISO 75-2/A | 112 °C | |
Linear coefficient of thermal expansion | 流动 | ASTM D696 | 0.000070 cm/cm/°C |
横动 | ASTM D696 | 0.000070 cm/cm/°C |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | 1.00 mm | UL 94 | V-1 无 |
1.50 mm | UL 94 | V-0 无 | |
2.00 mm | UL 94 | 5VB 无 |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Thermal performance | 测试条件 | 测试方法 | 属性值 单位 |
Surface Resistivity | IEC 60093 | 1000000000000000 ohms |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
melt mass-flow rate | 280℃/2.16 kg | ISO 1133 | 17 g/10 min |
shrinkage rate | 横向流量 : 4.00 mm | ISO 294-4 | 0.5-0.7 % |
流量 : 4.00 mm | ISO 294-4 | 0.5-0.7 % |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Water absorption rate | 23℃, 24 hr | ISO 62 | 0.22 % |
Tensile modulus | ISO 527-2/1 | 2350 Mpa | |
tensile strength | 屈服 | ISO 527-2/50 | 60 Mpa |
Elongation at break | ISO 527-2/50 | 100 % | |
ISO 527-2/50 | 50 % | ||
flexural modulus | ISO 178 | 2300 Mpa | |
bending strength | ISO 178 | 95 Mpa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.