PA66 Zytel® WRF403 NC010 DUPONT USA
175
- Unit Price:US$ 10,020 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:10MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:Glass fiber reinforced|High rigidity
- Application Areas:sporting goods|Automotive Applications
- Color:--
- Grade:Wear resistant grade
Technical Data Sheet
other | Test Condition | Test Method | Test Result |
---|---|---|---|
characteristic | PA66.30%玻纤增强.热稳定.高耐摩擦磨损 |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
bending strength | ASTM D790/ISO 178 | 270 kg·cm/cm(J/M)ft·lb/in | |
Bending modulus | ASTM D790/ISO 178 | 9200 kg·cm/cm(J/M)ft·lb/in | |
tensile strength | ASTM D638/ISO 527 | 185 kg/cm²(MPa)[Lb/in²] | |
Tensile modulus | ASTM D638/ISO 527 | 10300 kg/cm²(MPa)[Lb/in²] | |
Elongation at Break | ASTM D638/ISO 527 | 2.8 % | |
Charpy Notched Impact Strength | ASTM D256/ISO 179 | 80 kg·cm/cm(J/M)ft·lb/in | |
ASTM D256/ISO 179 | 13 kg·cm/cm(J/M)ft·lb/in | ||
(Dry) | ISO 179 | 11.0 kJ/m² | |
bending strength | (Dry) | ISO 178 | 270 Mpa |
Bending modulus | (Dry) | ISO 178 | 9200 Mpa |
Tensile modulus | (Dry) | ISO 527-1 | 10300 Mpa |
Tensile strain | (Dry),Break | ISO 527-1 | 2.8 % |
Tensile stress | (Dry),Break | ISO 527-1 | 185 Mpa |
Impact strength of cantilever beam gap | (Dry) | ISO 180 | 13.0 kJ/m² |
Suspended wall beam without notch impact strength | (Dry) | ISO 180 | 70.0 kJ/m² |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Melting temperature | 263 ℃(℉) | ||
Hot deformation temperature | HDT | ASTM D648/ISO 75 | 250 ℃(℉) |
1.80 Mpa,Unannealed(Dry) | ISO 75A-1 | 250 °C | |
Melting temperature | (Dry) | ISO 3146 | 263 °C |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Shrinkage rate | ASTM D955 | 0.3-0.8 % | |
density | ASTM D792/ISO 1183 | 1.50 | |
Shrinkage rate | (Dry),(Flow) | ISO 294-4 | 0.30 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.