PA66 Zytel® 80G14AHS-BK099 DUPONT USA
184
- Unit Price:US$ 6,530 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:20MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
For more details, please contact the supplier!
Material Description
- Material Properties:High impact resistance|Thermal stability|Filler: Glass fiber reinforced material|14% filler by weight
- Application Areas:Electrical applications|small home appliances
- Color:--
- Grade:Enhanced level
Material Certification

Technical Data Sheet
impact performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 55 kJ/m² |
Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 13 kJ/m² |
-40°C | ISO 180/1A | 6.0 kJ/m² | |
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 70 kJ/m² |
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 13 kJ/m² |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | 3.0mm | UL 94 | HB |
1.5mm | IEC 60695-11-10,-20 | HB | |
3.0mm | IEC 60695-11-10,-20 | HB | |
Extreme Oxygen Index | ISO 4589-2 | 21 % | |
FMVSS flammability | FMVSS302 | B | |
UL flame retardant rating | 1.5mm | UL 94 | HB |
Burning rate | 1.00mm | ISO 3795 | <100 mm/min |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Bending modulus | ISO 178 | 4400 Mpa | |
Tensile strain | Break | ISO 527-2 | 3.8 % |
tensile strength | Break | ISO 527-2 | 110 Mpa |
Tensile modulus | ISO 527-2 | 5000 Mpa |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Linear coefficient of thermal expansion | TD:55to160°C | ISO 11359-2 | 1.4E-04 cm/cm/°C |
TD:-40to23°C | ISO 11359-2 | 9.7E-05 cm/cm/°C | |
TD:-- | ISO 11359-2 | 1E-04 cm/cm/°C | |
MD:55to160°C | ISO 11359-2 | 4E-05 cm/cm/°C | |
MD:-40to23°C | ISO 11359-2 | 4E-05 cm/cm/°C | |
MD:-- | ISO 11359-2 | 4E-05 cm/cm/°C | |
Melting temperature | ISO 11357-3 | 263 °C | |
Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 240 °C |
0.45MPa,Unannealed | ISO 75-2/B | 258 °C |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Top out temperature | 210 °C | ||
density | ISO 1183 | 1.19 g/cm³ | |
Shrinkage rate | MD | ISO 294-4 | 0.70 % |
TD | ISO 294-4 | 0.90 % |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
Odor | VDA270 | 4.50 | |
EmissionofOrganicCompounds | VDA277 | 3.90 µgC/g |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.