Material Description
- Material Properties:Aging resistance|Weather resistance|Thermal stability
- Application Areas:Industrial applications
- Color:--
- Grade:Blow molding grade
Material Certification

Technical Data Sheet
Other performance | Test Condition | Test Method | Test Result |
---|---|---|---|
bending strength | ASTM D-1052 | >5×10 |
Basic Performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Water absorption rate | 24hr | ASTM D-570 | 0.5 % |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Elongation at Break | Break | ASTM D-638 | 40 Mpa |
Rubbing modulus | 23℃ | ASTM D-790 | 207 Mpa |
Initial tear strength | ASTM D-1004 | 158 kN/m | |
Elongation at Break | ASTM D-638 | 500 % | |
tensile strength | 10%伸长 | ASTM D-638 | 10.3 Mpa |
5%伸长 | ASTM D-638 | 6.9 Mpa | |
Shore hardness | ASTM D-2240 | 55 | |
Impact strength of cantilever beam gap | 23℃ | ASTM D-256 | 不破裂 J/m |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Hot deformation temperature | @0.18Mpa | ASTM D-648 | 49 °C |
Vicat softening temperature | ASTM D-1525 | 180 °C | |
Melting temperature | ASTM D-3418 | 203 °C |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Taber abraser | CS-17轮 | ASTM D-1044 | 6 mg/1000rev |
H 18轮 | ASTM D-1044 | 64 mg/1000rev | |
melt mass-flow rate | ASTM D-1238 | 7.5 g/10min | |
Hot deformation temperature | @0.5Mpa | ASTM D-648 | 90 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.