Thermal Properties | Test Condition | Test Method | DUPONT USA/5556 |
---|---|---|---|
Vicat Softening Temperature | ASTM D-1525 | 180 °C | |
Thermal distortion temperature | @0.18Mpa | ASTM D-648 | 49 °C |
Melting Temperature | ASTM D-3418 | 203 °C |
Physical | Test Condition | Test Method | DUPONT USA/5556 |
---|---|---|---|
Taber wear | CS-17轮 | ASTM D-1044 | 6 mg/1000rev |
Thermal distortion temperature | @0.5Mpa | ASTM D-648 | 90 °C |
Melt index | ASTM D-1238 | 7.5 g/10min | |
Taber wear | H 18轮 | ASTM D-1044 | 64 mg/1000rev |
Moisture Absorption (24hr) | ASTM D-570 | 0.5 % |
Mechanical Properties | Test Condition | Test Method | DUPONT USA/5556 |
---|---|---|---|
Durometer Hardness | ASTM D-2240 | 55 | |
Tearing Strength | ASTM D-1004 | 158 kN/m | |
Notched Izod Impact Strength | 23℃ | ASTM D-256 | 不破裂 J/m |
Tensile Strength | 5%伸长 | ASTM D-638 | 6.9 Mpa |
Tensile Elongation (Break) | ASTM D-638 | 500 % | |
Tensile Strength | 10%伸长 | ASTM D-638 | 10.3 Mpa |
Tensile Strength (Break) | ASTM D-638 | 40 Mpa | |
Tensile Modulus | 23℃ | ASTM D-790 | 207 Mpa |
Other | Test Condition | Test Method | DUPONT USA/5556 |
---|---|---|---|
Ross Flex | ASTM D-1052 | >5×10 |