plas

PC LEXAN™  EXL6013-88225 SABIC EU

218
  • Unit Price:US$ 3,429 /MT
  • Packaging Specification:
    25 KG/PKG
  • Packaging Material:
    Paper bag
  • Supply Quantity:
    20MT
  • Delivery Terms:
    FOB
  • Port of Loading :
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 ********View
serv********View
+86 ********View

For more details, please contact the supplier!

Material Description

  • Material Properties:High mobilityDuctility at low temperatureShort molding cycle
  • Application Areas:Electronic and Electrical ApplicationsAerospace Applicationslens
  • Color:--
  • Grade:Injection grade

Technical Data Sheet

impact performanceTest ConditionTest MethodTest Result
Charpy Notched Impact Strength-30°CISO 179/1eA70 kJ/m²
Charpy Notched Impact Strength23°CISO 179/1eA75 kJ/m²
Impact strength of simply supported beam without notch-30°CISO 179/1eU无断裂
Impact strength of simply supported beam without notch23°CISO 179/1eU无断裂
Impact strength of cantilever beam gap-30°CISO 180/1A60 kJ/m²
Impact strength of cantilever beam gap23°CISO 180/1A70 kJ/m²
Suspended wall beam without notch impact strength-30°CISO 180/1U无断裂
Suspended wall beam without notch impact strength23°CISO 180/1U无断裂
flammabilityTest ConditionTest MethodTest Result
UL flame retardant rating3.00mmUL 94V-1
Burning wire flammability index1.00mmIEC 60695-2-12850 °C
mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusISO 527-2/12100 Mpa
tensile strengthYieldISO 527-2/5055.0 Mpa
tensile strengthBreakISO 527-2/5060.0 Mpa
Tensile strainYieldISO 527-2/507.0 %
Tensile strainBreakISO 527-2/50100 %
Bending modulusISO 1782150 Mpa
bending strengthISO 17880.0 Mpa
Taber abraser1000Cycles,1000g,CS-17WheelInternal Method10.0 mg
thermal performanceTest ConditionTest MethodTest Result
Ball Pressure Test125°CIEC 60695-10-2Pass
Linear coefficient of thermal expansionMD:23to80°CISO 11359-27E-05 cm/cm/°C
Linear coefficient of thermal expansionTD:23to80°CISO 11359-27E-05 cm/cm/°C
thermal conductivityISO 83020.20 W/m/K
0.45MPa, unannealed, 100mm spanISO 75-2/Be131 °C
1.8MPa, unannealed, 100mm spanISO 75-2/Ae122 °C
Physical propertiesTest ConditionTest MethodTest Result
Water absorption rateEquilibrium,23°C,50%RHISO 620.15 %
Melt Volume Flow Rate (MVR)300°C/1.2kgISO 11335.50 cm3/10min
Shrinkage rateMD1Internal Method0.60-0.80 %
Water absorption rateSaturation,23°CISO 620.35 %
Electrical performanceTest ConditionTest MethodTest Result
Surface resistivityIEC 60093>1.0E+15 ohms
Volume resistivityIEC 60093>1.0E+15 ohms·cm
Dielectric strength3.20mm,in OilIEC 60243-117 KV/mm
Relative permittivity50HzIEC 602502.70
Relative permittivity60HzIEC 602502.70
Relative permittivity1MHzIEC 602502.70
Dissipation factor50HzIEC 602501E-03
Dissipation factor60HzIEC 602501E-03
Dissipation factor1MHzIEC 602500.010
Compared to the anti leakage trace indexIEC 60112PLC 3
hardnessTest ConditionTest MethodTest Result
Ball Pressure TestH358/30ISO 2039-190.0 Mpa
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.