Material Description
- Material Properties:Thermal stability|Carbon fiber reinforced
- Application Areas:Mechanical parts|consumer goods
- Color:--
- Grade:--
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Multi axis Instrumented Impact Energy | ISO 6603-2 | 5.00 J | |
| Dart impact | 23°C,EnergyatPeakLoad | ASTM D3763 | 7.00 J |
| Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 45 kJ/m² |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 7.3 kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| bending strength | ISO 178 | 425 Mpa | |
| ASTM D790 | 441 Mpa | ||
| Bending modulus | ISO 178 | 26600 Mpa | |
| ASTM D790 | 26800 Mpa | ||
| Tensile strain | Break | ISO 527-2 | 1.3 % |
| elongation | Break | ASTM D638 | 1.0 % |
| tensile strength | Break | ISO 527-2 | 232 Mpa |
| Break | ASTM D638 | 261 Mpa | |
| Tensile modulus | ISO 527-2/1 | 35500 Mpa | |
| ASTM D638 | 33800 Mpa |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed,64.0mmSpan | ISO 75-2/Af | >250 °C |
| 1.8MPa,Unannealed,3.20mm | ASTM D648 | >249 °C |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shrinkage rate | MD:24hr | ISO 294-4 | 0.70-0.90 % |
| TD:24hr | ISO 294-4 | 0.70-0.90 % | |
| TD:24hr | ASTM D955 | 0.70-0.90 % | |
| MD:24hr | ASTM D955 | 0.70-0.90 % | |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.46to1.4 % |
| 24hr,50%RH | ASTM D570 | 0.40 % |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Volume resistivity | ASTM D257 | 1.0E+2to1.0E+4 ohms·cm | |
| Surface resistivity | ASTM D257 | 1.0E+2to1.0E+4 ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.