PA6 Ultramid® B3S(粉) BASF SHANGHAI
248
- Unit Price:US$ 3,428 /MT
- Packaging Specification:25 KG/PKG
- Packaging Material:Paper bag
- Supply Quantity:40MT
- Delivery Terms:FOB
- Port of Loading :China Main Port
- Accepted Payment Methods:T/T
- Shipping:Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 ********View
serv********View
+86 ********View
For more details, please contact the supplier!
Material Description
- Material Properties:crystallization|High mobility|Fast forming cycle|Oil resistant
- Application Areas:Thin walled components|parts|Shell
- Color:--
- Grade:--
Technical Data Sheet
impact performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179 | 4.0 kJ/m² |
Impact strength of simply supported beam without notch | -30°C | ISO 179 | 200 kJ/m² |
23°C | ISO 179 | 250 kJ/m² | |
Impact strength of cantilever beam gap | 23°C | ISO 180 | 3.0 kJ/m² |
Charpy Notched Impact Strength | -30°C | ISO 179 | 3.0 kJ/m² |
mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | 23°C | ISO 527-2 | 3400 Mpa |
tensile strength | Yield,23°C | ISO 527-2 | 88.0 Mpa |
Tensile strain | Yield,23°C | ISO 527-2 | 3.8 % |
Nominal tensile fracture strain | 23°C | ISO 527-2 | 10 % |
Bending modulus | 23°C | ISO 178 | 2900 Mpa |
thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 65.0 °C |
Melting temperature | ISO 3146 | 220 °C |
Physical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183 | 1.13 g/cm³ | |
Melt Volume Flow Rate (MVR) | 275°C/5.0kg | ISO 1133 | 175 cm3/10min |
Water absorption rate | Saturation,23°C | ISO 62 | 9.5 % |
Equilibrium,23°C,50%RH | ISO 62 | 3.0 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.