PC/ABS CYCOLOY™  C3650-111 SABIC INNOVATIVE NANSHA

146
Unit Price:$4530 USD/MT
Packaging Specification:
25 KG/PKG
Supply Quantity:
30MT
Delivery Terms:
FOB
Port of Loading:
China Main Port
Accepted Payment Methods:
T/T
Shipping:
Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:High mobilityAging resistance
  • Application Areas:ShellElectronic and electrical
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

PhysicalTest ConditionTest MethodTest Result
Melt Mass-Flow Rate260°C/5.0kgASTMD12388.5 g/10min
Melt Volume flow Rate260°C/5.0kgISO11338.00 cm3/10min
Modeling ShrinkageMD:3.20mm内部方法0.40to0.60 %
Moisture Absorption饱和,23°CASTMD5700.60 %
Thermal PropertiesTest ConditionTest MethodTest Result
Linear thermal expansion coefficientMD:23到60°CISO11359-28E-05 cm/cm/°C
Linear thermal expansion coefficientTD:-40到40°CASTME8317.2E-05 cm/cm/°C
Linear thermal expansion coefficientTD:23to60°CISO11359-28E-05 cm/cm/°C
Thermal ConductivityISO83020.20 W/m/K
RTIElecUL74660.0 °C
Evolution Calendar intelligent importerUL74660.0 °C
RTIStrUL74660.0 °C
Heat Deflection Temperature0.45MPa,未退火,3.20mmASTMD648100 °C
Heat Deflection Temperature0.45MPa,Unannealed,100mmSpanISO75-2/Be102 °C
Heat Deflection Temperature1.8MPa,未退火,3.20mmASTMD64888.9 °C
Heat Deflection Temperature1.8MPa,Unannealed,100mmSpanISO75-2/Ae91.0 °C
Vicat Softening TemperatureASTMD152510110 °C
Vicat Softening Temperature--ISO306/B50108 °C
Vicat Softening Temperature--ISO306/B120110 °C
Linear thermal expansion coefficientMD:-40到40°CASTME8317.2E-05 cm/cm/°C
FlammabilityTest ConditionTest MethodTest Result
Flame Rating1.5mmUL94V-0
Flame Rating2.5mmUL945VB
Oxygen IndexISO4589-237 %
Electrical PropertiesTest ConditionTest MethodTest Result
Surface ResistivityIEC60093>1.0E+15 ohms
Volume ResistivityIEC60093>1.0E+15 ohms·cm
Dielectric Strength0.800mm,在油中IEC60243-135 KV/mm
Dielectric Strength1.60mm,在油中IEC60243-125 KV/mm
Dielectric Strength3.20mm,在油中IEC60243-117 KV/mm
Relative Permittivity50HzIEC602502.80
Relative Permittivity60HzIEC602502.80
Relative Permittivity1MHzIEC602502.70
Dissipation Factor?50HzASTMD1506E-03
Dissipation Factor?60HzASTMD1506E-03
Dissipation Factor?50HzIEC602504E-03
Dissipation Factor?60HzIEC602504E-03
Dissipation Factor?1MHzIEC602506E-03
Comparative Tracking IndexIEC60112600 V
Mechanical PropertiesTest ConditionTest MethodTest Result
Tensile ModulusASTMD6382860 Mpa
Tensile ModulusISO527-2/12600 Mpa
Tensile Strength屈服ASTMD63864.8 Mpa
Tensile Stress屈服ISO527-2/555.0 Mpa
Tensile Stress屈服ISO527-2/5065.0 Mpa
Flexural ModulusISO1782700 Mpa
Flexural StrengthISO178100 Mpa
Flexural Strength屈服,50.0mm跨距ASTMD790101 Mpa
Tensile Strength断裂ASTMD63851.0 Mpa
Tensile Stress断裂ISO527-2/550.0 Mpa
Tensile Stress断裂ISO527-2/5055.0 Mpa
Tensile Elongation屈服ASTMD6384.9 %
Tensile Strain屈服ISO527-2/53.0 %
Tensile Strain屈服ISO527-2/504.5 %
Tensile Elongation断裂ASTMD63835 %
Tensile Strain断裂ISO527-2/555 %
Tensile Strain断裂ISO527-2/50>50 %
Flexural Modulus50.0mm跨距ASTMD7902690 Mpa
HardnessTest ConditionTest MethodTest Result
Rockwell HardnessR级ISO2039-2124
Ball Indentation HardnessH358/30ISO2039-1113 Mpa
Impact PropertiesTest ConditionTest MethodTest Result
Charpy Notched Impact Strength-30°CISO179/1eA13 kJ/m²
Charpy Notched Impact Strength23°CISO179/1eA48 kJ/m²
Notched Izod Impact Strength-30°CISO180/1A13 kJ/m²
Notched Izod Impact Strength0°CISO180/1A15 kJ/m²
Notched Izod Impact Strength23°CISO180/1A45 kJ/m²
Instrumented Dart Impact23°C,TotalEnergyASTMD376365.0 J
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.