PC LEXAN™ 1800R SABIC INNOVATIVE US
119
Unit Price:$4604 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 20MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High gloss|Aging resistance|wear resistant|Weather resistance|Thermal stability
- Application Areas:Casters|Automotive sector|Household appliances|Electronic field|Electrical field
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical | Test Condition | Test Method | Test Result |
---|---|---|---|
Melt Mass-Flow Rate | 300°C/1.2kg | ASTMD1238 | 18 g/10min |
Melt Volume flow Rate | 300°C/1.2kg | ISO1133 | 17.0 cm3/10min |
Modeling Shrinkage | MD:--1 | 内部方法 | 0.50到0.70 % |
MD:3.20mm | 内部方法 | 0.50到0.70 % | |
Saturation ,23℃ | ISO62 | 0.35 % | |
ASTMD570 | 0.35 % |
Thermal Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
0.45MPa, Unannealed,3.20mm | ASTMD648 | 135 °C | |
0.45MPa, Unannealed,3.20mm Span | ISO75-2/Bf | 135 °C | |
1.8MPa, Unannealed,3.20mm | ASTMD648 | 124 °C | |
1.8MPa, Unannealed,64.0mm Span | ISO75-2/Af | 124 °C | |
Vicat Softening Temperature | ISO527-3/1 | 141 °C | |
Ball PressureTest | 125°C | IEC60695-10-2 | Pass |
-40到95°C | ASTME831 | 7E-05 cm/cm/°C | |
23到80°C | ISO11359-2 | 7E-05 cm/cm/°C | |
Thermal Conductivity | DENKA Method | 0.20 W/m/K |
Optical | Test Condition | Test Method | Test Result |
---|---|---|---|
Index of Refraction | ASTMD542,ISO489 | 1.586 | |
Transmittance | 2540µm | ASTMD1003 | 88.0到90.0 % |
Haze | 2540µm | ASTMD1003 | <0.80 % |
Flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Flame Rating | 1.50mm | UL94 | V-2 |
Mechanical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Yield,50.0mm Span | ASTMD790 | 90.0 Mpa | |
--2 | ASTMD638 | 2350 Mpa | |
Yield | ASTMD638 | 63.0 Mpa | |
yield | ISO527-2/50 | 63.0 Mpa | |
Yield | ASTMD638 | 6.0 % | |
yield | ISO527-2/50 | 6.0 % | |
Break | ASTMD638 | >70 % | |
fracture | ISO527-2/50 | >70 % | |
50.0mm Span | ASTMD790 | 2300 Mpa | |
--7 | ISO178 | 2300 Mpa | |
--8 | ISO178 | 90.0 Mpa |
Electrical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Dissipation Factor? | 60Hz | ASTMD150,IEC60250 | 1E-03 |
1MHz | ASTMD150,IEC60250 | 0.010 | |
Volume Resistivity | ASTMD257,IEC60093 | >1.0E+15 ohms·cm | |
Dielectric Strength | 1.60mm | ASTMD2863 | 27 KV/mm |
Dielectric Constant | 60Hz | ASTMD150,IEC60250 | 3.00 |
1MHz | ASTMD150,IEC60250 | 3.00 |
Hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Rockwell Hardness (R-Scale) | ASTMD785 | 120 | |
R-Scale | ISO2039-2 | 120 |
Impact Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
23°C | ASTMD256 | 700 J/m | |
-30°C10 | ISO180/1A | 12 kJ/m² | |
23°C11 | ISO180/1A | 70 kJ/m² | |
23°C | ASTMD4812,ISO180/1U | 无断裂 | |
-30°C12 | ISO180/1U | 无断裂 | |
Instrumented Dart Impact | 23°C,EnergyatPeakLoad | ASTMD3763 | 65.0 J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.