PC LEXAN™ 943 WH SABIC INNOVATIVE NANSHA
118
Unit Price:$2491 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 30MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Material Certification
Technical Data Sheet
Material Description
- Material Properties:Flame retardant|Easy to process|Impact modification|Bromine free
- Application Areas:Electrical appliances|Plastic bag|Electronic field|Electrical field
- Color:--
- Grade:Injection grade
Material Certification

Technical Data Sheet
Physical | Test Condition | Test Method | Test Result |
---|---|---|---|
Melt Mass-Flow Rate | 300°C/1.2kg | ASTMD1238 | 10 g/10min |
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.50to0.70 % |
Moisture Absorption | 24hr | ASTMD570 | 0.15 % |
平衡,23°C | ASTMD570 | 0.35 % | |
平衡,100°C | ASTMD570 | 0.58 % | |
Outdoor Suitability | UL746C | f1 | |
Specific Volume | ASTMD792 | 0.835 cm³/g |
Thermal Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat Deflection Temperature | 0.45MPa,未退火,6.40mm | ASTMD648 | 138 °C |
1.8MPa,未退火,6.40mm | ASTMD648 | 132 °C | |
Vicat Softening Temperature | ASTMD15255 | 152 °C | |
Linear thermal expansion coefficient | MD:-40到95°C | ASTME831 | 6.8E-05 cm/cm/°C |
Thermal Conductivity | ASTMC177 | 0.19 W/m/K | |
RTIElec | UL746 | 130 °C | |
Evolution Calendar intelligent importer | UL746 | 120 °C | |
RTIStr | UL746 | 130 °C |
Flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Flame Rating | 1.5mm | UL94 | V-0 |
Oxygen Index | ASTMD2863 | 35 % |
Mechanical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile Strength | 屈服 | ASTMD638 | 62.1 Mpa |
断裂 | ASTMD638 | 55.8 Mpa | |
Tensile Elongation | 屈服 | ASTMD638 | 7.0 % |
断裂 | ASTMD638 | 90 % | |
Flexural Modulus | 50.0mm跨距 | ASTMD790 | 2240 Mpa |
Flexural Strength | 屈服,50.0mm跨距 | ASTMD790 | 91.0 Mpa |
Taber Abrasion Resistance | 1000Cycles,1000g,CS-17转轮 | ASTMD1044 | 10.0 mg |
Electrical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Volume Resistivity | ASTMD257 | >1.0E+17 ohms·cm | |
Dielectric Strength | 3.20mm,inAir | ASTMD149 | 17 KV/mm |
Dielectric Constant | 50Hz | ASTMD150 | 3.01 |
60Hz | ASTMD150 | 3.01 | |
1MHz | ASTMD150 | 2.96 | |
Dissipation Factor? | 50Hz | ASTMD150 | 9E-04 |
60Hz | ASTMD150 | 9E-04 | |
1MHz | ASTMD150 | 0.010 | |
Arc Resistance | ASTMD495 | PLC7 | |
Comparative Tracking Index | CTI | UL746 | PLC 3 |
High Amp Arc Ignition | HAI | UL746 | PLC 2 |
High Voltage Arc Tracking Rate | HVTR | UL746 | PLC 3 |
Hot-wire Ignition | HWI | UL746 | PLC 1 |
Hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Rockwell Hardness | M计秤 | ASTMD785 | 70 |
R计秤 | ASTMD785 | 118 |
Impact Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Gardner Impact | 23°C | ASTMD3029 | 169 J |
Tensile Impact Strength | ASTMD1822 | 525 kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.