PC LNP™ LUBRICOMP™ DFL-4034 BK SABIC INNOVATIVE US
120
Unit Price:$5768 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 24MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Easy to demould|Easy to form
- Application Areas:Casters|Electronic and Electrical
- Color:--
- Grade:Injection grade
Technical Data Sheet
Physical | Test Condition | Test Method | Test Result |
---|---|---|---|
Modeling Shrinkage | MD:24小时 | ASTMD955 | 0.020到0.040 % |
TD:24小时 | ASTMD955 | 0.20到0.40 % | |
24hr,50%RH | ASTMD570 | 0.090 % | |
Equilibrium,23°C,50%RH | ISO62 | 0.13 % |
Thermal Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
0.45MPa, Unannealed,3.20mm | ASTMD648 | 146 °C | |
0.45MPa, Unannealed,3.20mm Span | ISO75-2/Bf | 146 °C | |
1.8MPa, Unannealed,3.20mm | ASTMD648 | 142 °C | |
1.8MPa, Unannealed,64.0mm Span | ISO75-2/Af | 141 °C | |
Linear thermal expansion coefficient | MD:-30到30°C | ASTMD696 | 3.7E-05 cm/cm/°C |
TD:-30到30°C | ASTMD696 | 6.3E-05 cm/cm/°C |
Mechanical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
--1 | ASTMD638 | 7190 Mpa | |
Break | ASTMD638 | 95.0 Mpa | |
fracture | ISO527-2/5 | 93.0 Mpa | |
Specific Wear Rate | Washer | ASTMD3702Modified | 89.0 10^-10in^5-min/ft-lb-hr |
yield | ISO527-2/5 | 2.8 % | |
Break | ASTMD638 | 2.7 % | |
fracture | ISO527-2/5 | 3.1 % | |
50.0mm Span | ASTMD790 | 6320 Mpa | |
--5 | ISO178 | 6200 Mpa | |
Break,50.0mm Span | ASTMD790 | 145 Mpa | |
Coefficient of Friction | 与自身-动态 | ASTMD3702Modified | 0.46 |
与自身-静态 | ASTMD3702Modified | 0.50 | |
Specific Wear Rate | Ring | ASTMD3702Modified | 13.0 10^-10in^5-min/ft-lb-hr |
Impact Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
23°C | ASTMD256 | 150 J/m | |
23°C7 | ISO180/1A | 14 kJ/m² | |
23°C | ASTMD4812 | 740 J/m | |
23°C8 | ISO180/1U | 49 kJ/m² | |
23°C,TotalEnergy | ASTMD3763 | 19.6 J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.