PC LEXAN™  3414R-731 SABIC INNOVATIVE US

123
Unit Price:$3059 USD/MT
Packaging Specification:
25 KG/PKG
Supply Quantity:
68MT
Delivery Terms:
FOB
Port of Loading:
China Main Port
Accepted Payment Methods:
T/T
Shipping:
Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Flame retardantenhanceGlass fiber reinforcedHigh rigidity
  • Application Areas:Fiber grade
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

PhysicalTest ConditionTest MethodTest Result
Modeling ShrinkageMD:3.20mm内部方法0.10to0.20 %
Moisture Absorption24hrASTMD5700.12 %
Moisture Absorption平衡,23°CASTMD5700.23 %
Specific VolumeASTMD7920.658 cm³/g
Melt Mass-Flow Rate300°C/5.0kgASTMD123813 g/10min
Thermal PropertiesTest ConditionTest MethodTest Result
RTIElecUL746130 °C
Evolution Calendar intelligent importerUL746130 °C
RTIStrUL746130 °C
Heat Deflection Temperature0.45MPa,未退火,6.40mmASTMD648154 °C
Heat Deflection Temperature1.8MPa,未退火,6.40mmASTMD648146 °C
Vicat Softening TemperatureASTMD15255166 °C
Linear thermal expansion coefficientMD:-40到95°CASTME8311.6E-05 cm/cm/°C
Specific HeatASTMC3511050 J/kg/°C
Thermal ConductivityASTMC1770.22 W/m/K
FlammabilityTest ConditionTest MethodTest Result
Flame Rating1.1mmUL94V-1
Flame Rating3.0mmUL94V-0
Mechanical PropertiesTest ConditionTest MethodTest Result
Tensile Strength断裂ASTMD638125 Mpa
Tensile Elongation断裂ASTMD6383.0 %
Flexural Modulus50.0mm跨距ASTMD7909650 Mpa
Flexural Strength屈服,50.0mm跨距ASTMD790186 Mpa
Taber Abrasion Resistance1000Cycles,1000g,CS-17转轮ASTMD104432.0 mg
Electrical PropertiesTest ConditionTest MethodTest Result
Volume ResistivityASTMD257>1.0E+17 ohms·cm
Dielectric Strength3.20mm,inAirASTMD14918 KV/mm
Dielectric Constant50HzASTMD1503.53
Dielectric Constant60HzASTMD1503.53
Dielectric Constant1MHzASTMD1503.48
Dissipation Factor?50HzASTMD1501.3E-03
Dissipation Factor?60HzASTMD1501.3E-03
Dissipation Factor?1MHzASTMD1506.7E-03
Arc ResistanceASTMD495PLC7
Comparative Tracking IndexCTIUL746PLC 4
High Amp Arc IgnitionHAIUL746PLC 4
High Voltage Arc Tracking RateHVTRUL746PLC 3
Hot-wire IgnitionHWIUL746PLC 0
HardnessTest ConditionTest MethodTest Result
Rockwell HardnessM计秤ASTMD78593
Rockwell HardnessR计秤ASTMD785119
Impact PropertiesTest ConditionTest MethodTest Result
Gardner Impact23°CASTMD30296.78 J
Tensile Impact StrengthASTMD182267.2 kJ/m²
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.