PA66 Zytel®  70G43HSLA BK099 DUPONT USA

118
Unit Price:$4469 USD/MT
Packaging Specification:
25 KG/PKG
Supply Quantity:
25MT
Delivery Terms:
FOB
Port of Loading:
China Main Port
Accepted Payment Methods:
T/T
Shipping:
Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:High mobilityLow crudThermal stability
  • Application Areas:Electronic and ElectricalAutomotive components
  • Color:--
  • Grade:--

Technical Data Sheet Compare

PhysicalTest ConditionTest MethodTest Result
Modeling Shrinkage横向流量ISO 294-40.90 %
Modeling Shrinkage流量ISO 294-40.30 %
Moisture Absorption24 hr, 23°C, 2.00 mmISO 620.90 %
Moisture Absorption饱和, 23°C, 2.00 mmISO 624.7 %
Moisture Absorption平衡, 23°C, 2.00 mm, 50% RHISO 621.5 %
Thermal PropertiesTest ConditionTest MethodTest Result
Heat Deflection Temperature0.45 MPa, 未退火ISO 75-2/B258 °C
Heat Deflection Temperature1.8 MPa, 未退火ISO 75-2/A255 °C
Glass Transition TemperatureISO 11357-280.0 °C
Melting TemperatureISO 11357-3262 °C
FlammabilityTest ConditionTest MethodTest Result
Burning Rate1.00 mmISO 379527 mm/min
Oxygen IndexISO 4589-224 %
FMVSS FlammabilityFMVSS 302B
Fill AnalysisTest ConditionTest MethodTest Result
Ejection Temperature210 °C
Thermal Conductivity of Melt0.25 W/m/K
Mechanical PropertiesTest ConditionTest MethodTest Result
Tensile ModulusISO 527-214000 Mpa
Tensile Stress断裂ISO 527-2225 Mpa
Tensile Strain断裂ISO 527-22.5 %
Flexural ModulusISO 17812500 Mpa
Flexural StressISO 178340 Mpa
Electrical PropertiesTest ConditionTest MethodTest Result
Volume ResistivityIEC 62631-3-1> 1.0E+13 ohms·m
Dielectric StrengthIEC 60243-125 KV/mm
Dissipation Factor?100 HzIEC 62631-2-10.013
Dissipation Factor?1 MHzIEC 62631-2-10.015
Comparative Tracking IndexIEC 60112600 V
InjectionTest ConditionTest MethodTest Result
Drying Temperature80 °C
Drying time - Hot air dryer2.0 到 4.0 hr
Suggested Max Moisture0.20 %
Processing (Melt) Temp285 到 300 °C
Melt Temperature, Optimum295 °C
Mold Temperature70 到 120 °C
Mold Temperature, Optimum100 °C
Holding Pressure50.0 到 100 Mpa
Holding PressureDrying Recommendedyes
Hold Pressure Time3.00 s/mm
Maximum Screw Tangential Speed12 m/min
Impact PropertiesTest ConditionTest MethodTest Result
Charpy Unnotched Impact Strength23°CISO 179/1eU90 kJ/m²
Multi-Axial Instrumented Impact Energy23°CISO 6603-24.40 J
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.