PA66 70G43HSLA BK099 DUPONT USA
Zytel® 
Electronic and Electrical、Automotive components
High mobility、Low crud、Thermal stability
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Thermal PropertiesTest ConditionTest MethodDUPONT USA/70G43HSLA BK099
Heat Deflection Temperature0.45 MPa, 未退火ISO 75-2/B258 °C
Melting TemperatureISO 11357-3262 °C
Heat Deflection Temperature1.8 MPa, 未退火ISO 75-2/A255 °C
Glass Transition TemperatureISO 11357-280.0 °C
Fill AnalysisTest ConditionTest MethodDUPONT USA/70G43HSLA BK099
Ejection Temperature210 °C
0.25 W/m/K
InjectionTest ConditionTest MethodDUPONT USA/70G43HSLA BK099
Drying time - Hot air dryer2.0 到 4.0 hr
Suggested Max Moisture0.20 %
Processing (Melt) Temp285 到 300 °C
3.00 s/mm
100 °C
Holding PressureDrying Recommendedyes
12 m/min
Holding Pressure50.0 到 100 Mpa
Drying Temperature80 °C
Mold Temperature70 到 120 °C
PhysicalTest ConditionTest MethodDUPONT USA/70G43HSLA BK099
Moisture Absorption平衡, 23°C, 2.00 mm, 50% RHISO 621.5 %
24 hr, 23°C, 2.00 mm0.90 %
Modeling Shrinkage横向流量ISO 294-40.90 %
流量0.30 %
Moisture Absorption饱和, 23°C, 2.00 mmISO 624.7 %
Mechanical PropertiesTest ConditionTest MethodDUPONT USA/70G43HSLA BK099
Tensile Strain断裂ISO 527-22.5 %
Tensile Modulus14000 Mpa
Tensile Stress断裂225 Mpa
Flexural ModulusISO 17812500 Mpa
Flexural Stress340 Mpa
Impact PropertiesTest ConditionTest MethodDUPONT USA/70G43HSLA BK099
Multi-Axial Instrumented Impact Energy23°CISO 6603-24.40 J
Charpy Unnotched Impact StrengthISO 179/1eU90 kJ/m²
FlammabilityTest ConditionTest MethodDUPONT USA/70G43HSLA BK099
FMVSS FlammabilityFMVSS 302B
Burning Rate1.00 mmISO 379527 mm/min
Oxygen IndexISO 4589-224 %
Electrical PropertiesTest ConditionTest MethodDUPONT USA/70G43HSLA BK099
Volume ResistivityIEC 62631-3-1> 1.0E+13 ohms·m
Dissipation Factor?100 HzIEC 62631-2-10.013
1 MHz0.015
Dielectric StrengthIEC 60243-125 KV/mm
Comparative Tracking IndexIEC 60112600 V