PPO NORYL™  PX1112-701 SABIC INNOVATIVE US

123
Unit Price:$4044 USD/MT
Packaging Specification:
25 KG/PKG
Supply Quantity:
10MT
Delivery Terms:
FOB
Port of Loading:
China Main Port
Accepted Payment Methods:
T/T
Shipping:
Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Dimensional stability Low Specific Gravity
  • Application Areas:Automotive body panels Automotive sector
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

物理性能Test ConditionTest MethodTest ResultUnit
吸水率饱和, 23°CISO 620.30%
吸水率平衡, 23°C, 50% RHISO 620.060%
熔体体积流动速率280°C/5.0 kgISO 11336.00cm3/10min
收缩率 - 流动  内部方法0.50 到 0.70%
机械性能Test ConditionTest MethodTest ResultUnit
弯曲应力 2, ISO 17870.0Mpa
悬壁梁缺口冲击强度 -30°CISO 180/1A10kJ/m²
悬壁梁缺口冲击强度 23°CISO 180/1A17kJ/m²
球压硬度H 358/30ISO 2039-180.0Mpa
泰伯耐磨性1000 Cycles, 1000 g, CS-17 转轮内部方法65.0mg
拉伸模量ISO 527-2/12100Mpa
拉伸强度屈服ISO 527-2/5040.0Mpa
拉伸强度断裂ISO 527-2/5040.0Mpa
伸长率屈服ISO 527-2/503.0%
伸长率断裂ISO 527-2/5030%
简支梁缺口冲击强度 -30°CISO 179/1eA10kJ/m²
简支梁缺口冲击强度 23°CISO 179/1eA17kJ/m²
弯曲模量 ISO 1781900Mpa
热性能Test ConditionTest MethodTest ResultUnit
维卡软化点--ISO 306/A50130°C
维卡软化点--ISO 306/B50120°C
维卡软化点--ISO 306/B120125°C
热变形温度0.45 MPa, 未退火, 4.00 mm, 100 mm 跨距ISO 75-2/Be120°C
热变形温度1.8 MPa, 未退火, 4.00 mm, 100 mm 跨距ISO 75-2/Ae105°C
导热系数ISO 83020.23W/m/K
线性热膨胀系数流动 : 23 到 80°CISO 11359-27.0E-5cm/cm/°C
线性热膨胀系数横向 : 23 到 80°CISO 11359-29.0E-5cm/cm/°C
Ball Pressure Test73 到 77°CIEC 60695-10-2通过
电气性能Test ConditionTest MethodTest ResultUnit
表面电阻率IEC 60093> 1.0E+15ohms
体积电阻率IEC 600931.0E+15ohms·cm
相对电容率50 HzIEC 602502.70
相对电容率60 HzIEC 602502.70
相对电容率1 MHzIEC 602502.60
耗散因数50 HzIEC 602504.0E-4
耗散因数60 HzIEC 602504.0E-4
耗散因数1 MHzIEC 602501.0E-3
注射Test ConditionTest MethodTest ResultUnit
干燥时间2.0 到 3.0hr
料筒后部温度240 到 260°C
料筒中部温度260 到 280°C
料筒前部温度280 到 300°C
射嘴温度260 到 280°C
料斗温度60 到 80°C
干燥温度100 到 120°C
加工(熔体)温度280 到 300°C
模具温度80 到 120°C
可燃性Test ConditionTest MethodTest ResultUnit
UL 阻燃等级1.6 mm, Testing by SABICUL 94HB
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.