TPU Texin® 285A COVESTRO USA
140
Unit Price:$8527 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 30MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:--
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
density | ASTM D792 | 1.2 | g/cm³ | |
ISO 1183 | 1.2 | g/cm³ | ||
Shrinkage rate | Flow2.5mm | ASTM D955 | 0.8 | % |
垂直2.5mm | ASTM D955 | 0.8 | % | |
垂直2.5mm | ISO 2577 | 0.8 | % | |
Flow2.5mm | ISO 2577 | 0.8 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Bending modulus | -30℃ | ISO 178 | 49.6 | Mpa |
23℃ | ASTM D790 | 27.6 | Mpa | |
Tiber wear and tear | H-18轮1kg 1000次循环 | ASTM D1044 | 35 | mg |
H-18轮1kg 1000次循环 | ISO 4649 | 35 | mg | |
tensile strength | 50%Strain | ISO 37 | 5 | Mpa |
100%Strain | ASTM D412 | 5.3 | Mpa | |
300%Strain | ASTM D412 | 13.1 | Mpa | |
Yield | ASTM D412 | 37.9 | Mpa | |
Yield | ISO 37 | 37.9 | Mpa | |
elongation | Break | ASTM D412 | 500 | % |
Break | ISO 37 | 500 | % | |
Tear Man apart | C型 | ASTM D624 | 87.6 | kN/m |
tear strength | ISO 34 | 87.6 | kN/m | |
Compression deformation | 23℃ 22hr | ISO 815 | 16 | % |
23℃ 22hr在110℃下后固化16hr | ASTM D395 | 12 | % | |
70℃ 22hr | ASTM D395 | 65 | % | |
70℃ 22hr在110℃下后固化16hr | ASTM D395 | 35 | % | |
Bayshore Elasticity | ASTM D2632 | 45 | % | |
compressive strength | 10%Strain | ASTM D575 | 2.24 | Mpa |
15%Strain | ASTM D575 | 3.28 | Mpa | |
2%Strain | ASTM D575 | 0.345 | Mpa | |
20%Strain | ASTM D575 | 4.31 | Mpa | |
25%Strain | ASTM D575 | 5.69 | Mpa | |
5%Strain | ASTM D575 | 1.03 | Mpa | |
50%Strain | ASTM D575 | 15 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Brittle temperature | ASTM D746 | -68 | °C | |
ISO 974 | -68 | °C | ||
Glass transition temperature | DMA | -42 | °C | |
vicat softening point | 50℃/hr | ISO 306 | 91 | °C |
50℃/hr | ASTM D1525 | 91 | cm/cm/℃ |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Fire rating | 1.5mm | UL94 | HB | |
3.0mm | UL95 | V-2 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.
Contact Us
Get App
Top