For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:--
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
density | ASTMD792 | 1.02 | g/cm³ | |
ISO1183 | 1.02 | g/cm³ | ||
Melt mass flow rate | 200°C/5.0kg | ASTMD1238 | 11 | g/10min |
Melt Volume-Flow Rate (MVR) | 200°C/5.0kg | ISO1133 | 12.0 | cm3/10min |
Shrinkage rate | MD | ASTMD955 | 0.65 | % |
ISO294-4 | 0.30to1.0 | % | ||
Water absorption rate | Saturation,23°C | ASTMD570 | 0.070 | % |
Saturation,23°C | ISO62 | 0.070 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | ASTMD638 | 1640 | Mpa | |
ISO527-2 | 1550 | Mpa | ||
tensile strength | Yield,23°C | ASTMD638 | 25.5 | Mpa |
Yield,23°C | ISO527-2 | 27.0 | Mpa | |
elongation | Yield,23°C | ISO527-2 | 2.0 | % |
Break | ASTMD638 | 220 | % | |
Nominal tensile fracture strain | 23°C | ISO527-2 | 180 | % |
Bending modulus | ASTMD790 | 1330 | Mpa | |
ISO178 | 1550 | Mpa | ||
bending strength | ASTMD790 | 27.2 | Mpa | |
5.0%Strain | 31.0 | Mpa | ||
-- | ISO178 | 31.0 | Mpa | |
Charpy Notched Impact Strength | 23°C | ISO179 | 3.0 | kJ/m² |
Impact strength of simply supported beam without notch | 23°C | ISO179 | NoBreak | |
Impact strength of cantilever beam gap | 23°C | ASTMD256 | 32 | J/m |
-30°C | ISO180/A | 2.0 | kJ/m² | |
23°C | ISO180/A | 3.0 | kJ/m² | |
InstrumentedDartImpact | Totalenergy | ASTMD3763 | 20.1 | J |
Shore hardness | Shore D | ASTMD2240 | 75 | |
Shore D | ISO868 | 65 |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa,Unannealed | ASTMD648 | 75.6 | °C |
0.45MPa,Annealed | ISO75-2/B | 75.0 | °C | |
1.8MPa,Unannealed | ASTMD648 | 60.0 | °C | |
1.8MPa,Annealed | ISO75-2/A | 58.0 | °C | |
vicat softening point | ASTMD15253 | 87.8 | °C | |
-- | ISO306/A50 | 81.0 | °C | |
-- | ISO306/B50 | 51.0 | °C | |
Linear coefficient of thermal expansion | MD | ASTMD696 | 1.3E-04 | cm/cm/°C |
MD | ISO11359-2 | 6.0E-5to9.0E-5 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface resistivity | ASTMD257 | >1.0E+14 | ohms | |
IEC60093 | 1E+15 | ohms | ||
Volume resistivity | ASTMD257 | >1.0E+15 | ohms·cm | |
IEC60093 | >1.0E+15 | ohms·cm | ||
Dielectric constant | 1.00mm,1MHz | ASTMD150 | 2.50 | |
100Hz | IEC60250 | 2.50 | ||
Dissipation factor | 100Hz | IEC60250 | 3E-04 | |
1MHz | IEC60250 | 8E-04 | ||
Leakage Trace Index | IEC60112 | 600 | V |
film | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Elongation MD | Break | ISO527-3 | 180 | % |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Haze | ASTMD1003 | 0.20 | % | |
Refractive index | ASTMD542 | 1.573 | ||
ISO489 | 1.573 | |||
Light transmittance | 550nm | ASTMD1003 | 91.0 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.