PBT Cristin®  HR5330HF-NC010 DUPONT USA

163
Unit Price:$5949 USD/MT
Packaging Specification:
25 KG/PKG
Supply Quantity:
10MT
Delivery Terms:
FOB
Port of Loading:
China Main Port
Accepted Payment Methods:
T/T
Shipping:
Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Hydrolysis resistance Glass fiber reinforced Filler: Glass fiber reinf 30% filler by weight
  • Application Areas:Electronic and electrical
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

物理性能Test ConditionTest MethodTest ResultUnit
收缩率TDISO294-41.0%
收缩率MDISO294-40.30%
吸水率饱和,23°C,2.00mmISO620.35%
吸水率平衡,23°C,2.00mm,50%RHISO620.15%
MeltDensity1.29g/cm³
顶出温度170°C
SpecificHeatCapacityofMelt1730J/kg/°C
ThermalConductivityofMelt0.28W/m/K
粘数ISO30795.0cm³/g
FlowLength2.00mm350mm
密度ISO11831.50g/cm³
密度ISO 11831.5g/cm
机械性能Test ConditionTest MethodTest ResultUnit
Charpy 非缺口冲击强度23 ℃, Type 1, EdgewiseISO 179KJ/m
简支梁无缺口冲击强度23°CISO179/1eU70kJ/m²
泊松比ISO5270.34
简支梁缺口冲击强度-,-30 ℃, Type 1, Edgewise, Notch AISO 17911.5KJ/m
简支梁缺口冲击强度-,23 ℃, Type 1, Edgewise, Notch AISO 179KJ/m
简支梁缺口冲击强度-30°CISO179/1eA12kJ/m²
简支梁缺口冲击强度23°CISO179/1eA13kJ/m²
悬壁梁缺口冲击强度-40°CISO180/1A11kJ/m²
悬壁梁缺口冲击强度23°CISO180/1A14kJ/m²
悬臂梁无缺口冲击强度23°CISO180/1U65kJ/m²
屈服点拉伸应力23℃ISO 527-1, -2134Mpa
屈服点拉伸应变23℃ISO 527-1, -2%
缺口冲击强度-,-40 ℃, Type 1, Notch AISO 180KJ/m
缺口冲击强度-,23 ℃, Type 1, Notch AISO 180KJ/m
拉伸模量23℃ISO 527-1, -28500Mpa
拉伸模量ISO527-28500Mpa
拉伸强度断裂ISO527-2132Mpa
伸长率断裂ISO527-23.5%
弯曲模量ISO1787700Mpa
弯曲模量23℃ISO 178Mpa
弯曲强度23℃ISO 178Mpa
弯曲强度ISO178200Mpa
热性能Test ConditionTest MethodTest ResultUnit
维卡软化点ISO306/B50215°C
线性热膨胀系数TD:55to160°CISO11359-21.5E-04cm/cm/°C
线性热膨胀系数MD:--ISO11359-22E-05cm/cm/°C
线性热膨胀系数MD:-40to23°CISO11359-22.5E-05cm/cm/°C
线性热膨胀系数MD:55to160°CISO11359-21.5E-05cm/cm/°C
线性热膨胀系数TD:--ISO11359-21.5E-04cm/cm/°C
线性热膨胀系数TD:-40to23°CISO11359-29E-05cm/cm/°C
熔融温度ISO11357-3225°C
熔融温度ISO 3146225
热变形温度-,0.45 Mpa,未退火
热变形温度-,1.80 Mpa,未退火
热变形温度0.45MPa,未退火ISO75-2/B221°C
热变形温度1.8MPa,未退火ISO75-2/A207°C
电气性能Test ConditionTest MethodTest ResultUnit
介电强度--IEC60243-144KV/mm
介电强度1.00mm5IEC60243-131KV/mm
相对电容率100HzIEC602504.40
相对电容率1MHzIEC602504.10
漏电起痕指数IEC60112450V
表面电阻率IEC600931E+13ohms
体积电阻率IEC60093>1.0E+15ohms·cm
耗散因数100HzIEC602502.5E-03
耗散因数1MHzIEC602500.020
耗散因数100HzASTMD1502.5E-03
耗散因数1kHzASTMD1507E-03
耗散因数1MHzASTMD1500.020
可燃性Test ConditionTest MethodTest ResultUnit
FlameRating0.75mmUL94HB
极限氧指数ISO4589-219%
FMVSS可燃性FMVSS302B
可燃性等级0.75mmIEC60695-11-10,-20HB
燃烧速率1.00mmISO379530mm/min
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.