۱٬۰۰۰ محصول

تولیدکننده: 意大利Taro Plast
حذف تمام فیلترها
موادتوصیف موادگواهی‌نامه‌هاقیمت مرجععملیات
TPV Taro Plast S.p.A. TAROPRENE® 1 A50 M1N
melt mass-flow rate 2.5 tensile strength 2.80
-- --
PBT Taro Plast S.p.A. TAROLOX 10 G3 X0
tensile strength 95.0 elongation 4.0 Hot deformation temperature 210
-- --
PP Homopolymer Taro Plast S.p.A. HAIPLEN H50 T5
melt mass-flow rate 10 Impact strength of cantilever beam gap 30 Hot deformation temperature 125 tensile strength 30.0 Filler Taro Plast Italian Taro Plast
-- --
PC+PBT Taro Plast S.p.A. TAROLOY 10
melt mass-flow rate 20 Impact strength of cantilever beam gap 700 Hot deformation temperature 110 tensile strength 60.0
-- --
PC Taro Plast S.p.A. TAROBLEND 85
Hot deformation temperature 128 melt mass-flow rate 23.0 tensile strength 55.0
-- --
PA6 Taro Plast S.p.A. TAROMID B 280 Z3
Water absorption rate 6.0 tensile strength 55.0 Hot deformation temperature 60.0 Bending modulus 1600
-- --
PC+ABS Taro Plast S.p.A. TAROBLEND 88 G2
melt mass-flow rate 12 Impact strength of cantilever beam gap 90 Hot deformation temperature 120 tensile strength 70.0 Filler glass fiber reinforced material 10% filler by weight
-- --
PC Taro Plast S.p.A. TAROLON 2011
Impact strength of cantilever beam gap 500 Hot deformation temperature 135 melt mass-flow rate 22 tensile strength 60.0 Thin walled components
-- --
PP Homopolymer Taro Plast S.p.A. NILENE® P6 K30VA
melt mass-flow rate 6.0 Impact strength of cantilever beam gap 130 Hot deformation temperature 156 tensile strength 90.0 Filler glass fiber reinforced material 30% filler by weight
-- --
PP Taro Plast S.p.A. NILENE® P K30VA V0
melt mass-flow rate 5.0 Impact strength of cantilever beam gap 65 Bending modulus 6500 tensile strength 70.0 Filler glass fiber reinforced material 30% filler by weight
-- --
PP Copolymer Taro Plast S.p.A. HAIPLEN EP60 T5
melt mass-flow rate 16 Impact strength of cantilever beam gap 30 Hot deformation temperature 130 tensile strength 30.0 Filler Taro Plast Italian Taro Plast
-- --
PP Copolymer Taro Plast S.p.A. HAIPLEN EP100 CM5
melt mass-flow rate 20 Impact strength of cantilever beam gap >300 Hot deformation temperature 64.0 tensile strength 18.0 Filler mineral filler 25% filler by weight Automotive internal components
-- --
ABS Taro Plast S.p.A. TARODUR 100 G3
Impact strength of cantilever beam gap 60 melt mass-flow rate 8.0 Hot deformation temperature 96.0 tensile strength 78.0 Filler glass fiber reinforced material 17% filler by weight
-- --
PP Copolymer Taro Plast S.p.A. HAIPLEN EP50 T7
melt mass-flow rate 10 Impact strength of cantilever beam gap 35 Hot deformation temperature 60.0 tensile strength 35.0 Filler talc filler 35% filler by weight
-- --
TPV Taro Plast S.p.A. TAROPRENE® 2 A65 E1G
melt mass-flow rate 5.0 tensile strength 2.25 shell
-- --
PP Homopolymer Taro Plast S.p.A. NILENE® P15 K30C
melt mass-flow rate 15 Impact strength of cantilever beam gap 35 Hot deformation temperature 125 tensile strength 30.0 Filler calcium carbonate filler 30% filler by weight
-- --
ASA Taro Plast S.p.A. TAROLOX 200 G2
Impact strength of cantilever beam gap 45 melt mass-flow rate 8.0 Hot deformation temperature 145 tensile strength 65.0 Filler glass fiber reinforced material 10% filler by weight
-- --
PP Taro Plast S.p.A. NILFLEX® 14 K10T
melt mass-flow rate 14 Impact strength of cantilever beam gap 400 Bending modulus 1350 tensile strength 25.0
-- --
PA66 Taro Plast S.p.A. TAROMID A 280 G3 K3
Water absorption rate 5.3 tensile strength 100 Hot deformation temperature 217 Bending modulus 5400 Filler glass bead glass fiber 30% filler by weight
-- --
PP Copolymer Taro Plast S.p.A. NILENE® E15 K20TE
melt mass-flow rate 15 Impact strength of cantilever beam gap 30 Hot deformation temperature 125 tensile strength 27.0 Filler mineral filler 20% filler by weight
-- --