برگه داده فنی
physical property | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
vicat | ISO 306/B50 | 110 °C | |
density | -- | ASTM D792 | 1.08 g/cm³ |
شرایط آزمون | روش آزمون | نتیجه آزمون | |
---|---|---|---|
tensile strength | -- | ISO 527-2/50 | 50.0 MPa |
elongation | Break | ASTM D638 | 60 % |
Flexural modulus | -- | ASTM D790 | 1900 MPa |
--2 | ISO 178 | 2000 MPa | |
Charpy Notched Impact Strength | 23°C | ISO 179 | 48 kJ/m² |
Impact strength of simply supported beam without notch | 23°C | ISO 179 | 无断裂 |
Impact strength of cantilever beam gap | 3.20mm | ASTM D256 | 500 J/m |
23°C4 | ISO 180 | 45 kJ/m² | |
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | 100 °C |
bending strength | -- | ASTM D790 | 70.0 MPa |
--2 | ISO 178 | 63.0 MPa | |
Charpy Notched Impact Strength | -30°C | ISO 179 | 32 kJ/m² |
density | -- | ISO 1183 | 1.12 g/cm³ |
melt mass-flow rate | 230°C/10.0kg | ASTM D1238 | 20 g/10min |
Shrinkage rate | MD | ASTM D955 | 0.50to0.70 % |
-- | ISO 294-4 | 0.50to0.70 % | |
tensile strength | -- | ASTM D638 | 53.0 MPa |
Surface Resistivity | IEC 60093 | >1.0E+15 ohms | |
Volume resistivity | IEC 60093 | >1.0E+15 ohms·cm |
Thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火5,HDT | ISO 75-2/A | 96.0 °C |