physical property | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Water absorption rate | 饱和,23°C | ISO 62 | 3.4 % |
density | | ASTM D792 | 1.58 g/cm³ |
density | | ISO 1183 | 1.58 g/cm³ |
Shrinkage rate | MD | ASTM D955 | 0.10to0.30 % |
Shrinkage rate | | ISO 294-4 | 0.10to0.30 % |
Water absorption rate | Saturation | ASTM D570 | 3.4 % |
Water absorption rate | Equilibrium | ASTM D570 | 1.0 % |
Water absorption rate | 平衡,23°C,50%RH | ISO 62 | 1.0 % |
flammability | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
UL flame retardant rating | 3.0mm | UL 94 | HB |
Mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
bending strength | | ASTM D790 | 380 MPa |
bending strength | | ISO 178 | 380 MPa |
tensile strength | Yield | ISO 527-2 | 230 MPa |
elongation | Break | ASTM D638 | 1.5 % |
Tensile strain | Break | ISO 527-2 | 1.5 % |
Flexural modulus | | ASTM D790 | 16500 MPa |
Flexural modulus | | ISO 178 | 16500 MPa |
Tensile modulus | | ISO 527-2 | 18000 MPa |
tensile strength | Yield | ASTM D638 | 230 MPa |
Tensile modulus | | ASTM D638 | 1800 MPa |
Impact resistance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Charpy Notched Impact Strength | 23°C | ISO 179 | 28 kJ/m² |
Impact strength of simply supported beam without notch | 23°C | ISO 179 | 100 kJ/m² |
Impact strength of cantilever beam gap | 23°C | ASTM D256 | 250 J/m |
Impact strength of cantilever beam gap | 23°C | ISO 180 | 25 kJ/m² |
Thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | 253 °C |
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 253 °C |