Ether Neostar™ FN006 Eastman Chemical Company

0

برگه داده فنی

impact performanceشرایط آزمونروش آزموننتیجه آزمون
Impact strength of cantilever beam gap-40°CASTM D25640 J/m
elastomerشرایط آزمونروش آزموننتیجه آزمون
Kappa modulus-28°CASTM D1043240 MPa
Kappa modulus-70°CASTM D1043930 MPa
mechanical propertiesشرایط آزمونروش آزموننتیجه آزمون
Bending modulus23°CASTM D790150 MPa
elongationBreak,23°CASTM D638400 %
elongationYield,23°CASTM D63838 %
tensile strengthBreak,23°C,2.00mm4ASTM D63822.0 MPa
tensile strengthYield,23°C,3.00mm,Injection3ASTM D63814.0 MPa
Tensile modulus23°CASTM D638170 MPa
thermal performanceشرایط آزمونروش آزموننتیجه آزمون
Brittle temperatureASTM D746<-75.0 °C
specific heat225°C8DSC2300 J/kg/°C
thermal conductivity23°CASTMC1770.19 W/m/K
Fusion temperature23°CASTME79327.0 kJ/kg
specific heat200°C7DSC3100 J/kg/°C
specific heat175°C6DSC2300 J/kg/°C
specific heat150°C6DSC2000 J/kg/°C
specific heat100°C6DSC1800 J/kg/°C
specific heat25°C6DSC1600 J/kg/°C
Crystallization peak temperatureDSCDSC140 °C
Melting temperatureASTM D3418205 °C
Vicat softening temperatureASTM D15255170 °C
Glass transition temperatureDSC-3.00 °C
Linear coefficient of thermal expansionMD:23°CASTM D6961.5E-04 cm/cm/°C
Physical propertiesشرایط آزمونروش آزموننتیجه آزمون
Intrinsic viscosity23°CInternal Method1.2
Water absorption rate23°C,24hrASTM D5700.40 %
melt mass-flow rate230°C/2.16kgASTM D123810 g/10min
densityASTM D7921.13 g/cm³
hardnessشرایط آزمونروش آزموننتیجه آزمون
Shore hardnessShoreD,23°CASTM D224055
Shore hardnessShoreA,23°CASTM D224095
Supplementary Informationشرایط آزمونروش آزموننتیجه آزمون
tear strength23°CASTM D1004350 N