impact performanceشرایط آزمونروش آزموننتیجه آزمون
Charpy Notched Impact Strength23°CISO 179/1eA10 kJ/m²
Impact strength of cantilever beam gap23°C,3.18mmASTM D25688 J/m
Impact strength of cantilever beam gap23°C,6.35mmASTM D25669 J/m
Impact strength of cantilever beam gap23°CISO 180/1A10 kJ/m²
mechanical propertiesشرایط آزمونروش آزموننتیجه آزمون
tensile strengthYieldASTM D638140 MPa
Tensile modulusISO 527-2/508800 MPa
Tensile modulusASTM D6388400 MPa
Tensile strainBreakISO 527-2/503.0 %
elongationBreakASTM D6383.0 %
tensile strengthBreakISO 527-2/50160 MPa
tensile strengthBreakASTM D638140 MPa
tensile strengthYieldISO 527-2/50159 MPa
Bending modulusASTM D7905900 MPa
bending strengthISO 178210 MPa
bending strengthASTM D790240 MPa
Bending modulusISO 17811000 MPa
thermal performanceشرایط آزمونروش آزموننتیجه آزمون
Vicat softening temperatureISO 306/B50248 °C
Hot deformation temperature1.8MPa,Unannealed,4.00mmISO 75-2/A234 °C
Hot deformation temperature1.8MPa,Unannealed,6.40mmASTM D648231 °C
Hot deformation temperature0.45MPa,Unannealed,4.00mmISO 75-2/B254 °C
Hot deformation temperature0.45MPa,Unannealed,6.40mmASTM D648250 °C
Physical propertiesشرایط آزمونروش آزموننتیجه آزمون
densityASTM D7921.24 g/cm³
Shrinkage rateMD:3.20mmISO 25770.40to0.49 %
Shrinkage rateTD:3.20mmISO 25770.50to0.61 %
Shrinkage rateTD:3.20mmASTM D9550.50to0.61 %
Shrinkage rateMD:3.20mmASTM D9550.40to0.49 %
melt mass-flow rate285°C/5.0kgISO 113320 g/10min
melt mass-flow rate285°C/5.0kgASTM D123820 g/10min
densityISO 11831.24 g/cm³
hardnessشرایط آزمونروش آزموننتیجه آزمون
Rockwell hardnessR-ScaleASTM D785117
Rockwell hardnessR-ScaleISO 2039-2117