برگه داده فنی
physical property | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
melt mass-flow rate | 190℃/2.16Kg | ASTM D1238 | 0.80 g/10min |
190℃/2.16kg | ASTM D-1238 | 0.80 g/10min | |
film thickness | DSC |
optical performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
Haze ratio | ASTM D1003 | 9.0 % |
Mechanical properties | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
tensile strength | ASTM D882 | 13 Mpa | |
断裂 | ASTM D882 | 29 Mpa | |
断裂 | ASTM D882 | 22 Mpa | |
elongation at break | ASTM D882 | 400 % | |
ASTM D882 | 610 % | ||
coefficient of friction | ASTM D-1894 | 0.45 | |
Dart impact | 35µm | ASTM D-1709 | 74 g |
tensile strength | 屈服,TD | 13 | |
MD,35µm,断裂 | ASTM D-882A | 29 MPa | |
TD,断裂 | 22 | ||
Secant modulus | MD,35µm,1%应变 | ASTM D-882 | 230 MPa |
TD,1%应变 | 270 | ||
elongation at break | MD,35µm | ASTM D-882 | 400 % |
TD | 610 |
Thermal performance | شرایط آزمون | روش آزمون | نتیجه آزمون |
---|---|---|---|
vicat | ASTM1525 | 99.8 °C |