AS(SAN) Luran® 368R 77851

63

برگه داده فنی

physical property شرایط آزمونروش آزموننتیجه آزمون
Disassembly rate1.569
Shrinkage rate0.3-0.7 %
Melting temperature range for pipeline extrusion220-240 °C
Water absorption rate0.2 %
melt mass-flow rate200/21 612
melt mass-flow rate220/1010
Melting temperature range for injection molding220-270 °C
Mold temperature range40-80 °C
Mechanical propertiesشرایط آزمونروش آزموننتیجه آزمون
Charpy Notched Impact Strength23℃2 KJ/m
Rockwell hardness83 M
Impact strength of cantilever beam gap23℃2 KJ/m
ball-indentation hardness165 Mpa
Breaking stress75 Mpa
Tensile stress屈服125 Mpa
elongation3 %
Tensile modulus3800 Mpa
Charpy Notched Impact Strength+23/-40℃18/18 KJ/m
Tensile creep modulus1000h 伸长率<=0.5%+23℃2800 Mpa
Electrical performanceشرایط آزمونروش آزموننتیجه آزمون
Relative Arc Track Index CTI Test Solution试验溶液A/CTIMCTI 425
dielectric constant100Hz/1MHz3/2.7
Volume resistivity10 Ω.cm
Surface Resistivity10 Ω
Relative Arc Track Index CTI Test Solution试验溶液BCTI 200M
dielectric strengthK20/P2095 KV/mm
loss angle100Hz/1MHz0.004/0.007
Thermal performanceشرایط آزمونروش آزموننتیجه آزمون
Heat distortion temperature0.45MPa(HDT B)102 °C
maximum service temperature85 °C
Heat distortion temperature1.8MPa(HDT A)98 °C
Conductivity0.17 W/K.m
Linear coefficient of thermal expansion纵向(23-80)℃7
vicat106 °C