شرایط آزمون | روش آزمون | نتیجه آزمون | |
---|---|---|---|
density | ASTM D792 | 2.14 g/cm³ | |
Volume resistivity | ASTM D257 | 1E+18 ohms·cm | |
ISO 1325 | 1E+18 ohms·cm | ||
dielectric strength | 0.250mm | ASTM D149 | 80 kV/mm |
melt mass-flow rate | 372°C/5.0kg | ASTM D3307 | 7.0 g/10min |
372°C/5.0kg | ISO 12086 | 7.0 g/10min | |
Water absorption rate | 24hr | ASTM D570 | <0.030 % |
tensile strength | 23°C | ASTM D3307 | 28.0 MPa |
200°C | ASTM D3307 | 13.0 MPa | |
23°C | ISO 12086 | 28.0 MPa | |
200°C | ISO 12086 | 13.0 MPa | |
elongation | 断裂,23°C | ASTM D3307 | 290 % |
dielectric strength | 0.250mm | IEC 60243-1 | 80 kV/mm |
dielectric constant | 1MHz | ASTM D150 | 2.03 |
1MHz | IEC 60250 | 2.03 | |
Dissipation Factor | 1MHz | ASTM D150 | <2.0E-4 |
1MHz | IEC 60250 | <2.0E-4 | |
UL flame retardant rating | UL 94 | V-0 | |
Limiting Oxygen Index | ASTM D2863 | >95 % | |
elongation | 断裂,200°C | ASTM D3307 | 450 % |
Tensile strain | 断裂,23°C | ISO 12086 | 290 % |
断裂,200°C | ISO 12086 | 450 % | |
Flexural modulus | 23°C | ASTM D790 | 600 MPa |
200°C | ASTM D790 | 55.0 MPa | |
23°C | ISO 178 | 600 MPa | |
200°C | ISO 178 | 55.0 MPa | |
Shore hardness | 邵氏D | ASTM D2240 | 55 |
邵氏D | ISO 868 | 55 | |
melting temperature | ASTM D4591 | 290 °C | |
Limiting Oxygen Index | ISO 4589-2 | >95 % | |
critical shear rate | 372°C | 21.0 sec^-1 | |
MITFoldingEndurance | 200.0µm | ASTM D2176 | 8E+05 Cycles |