برگه داده فنی مقایسهelastomer شرایط آزمون روش آزمون نتیجه آزمون Permanent compression deformation 70°C,22hr ASTM D395B 80 % Permanent compression deformation 25°C,22hr ASTM D395B 30 % tear strength 3.20mm ASTM D624 105 kN/m elongation Break,3.20mm ASTM D412 450 % tensile strength Break,3.20mm ASTM D412 38.9 Mpa tensile strength 300%Strain,3.20mm ASTM D412 21.4 Mpa tensile strength 100%Strain,3.20mm ASTM D412 9.70 Mpa tensile strength 50%Strain,3.20mm ASTM D412 8.30 Mpa
mechanical properties شرایط آزمون روش آزمون نتیجه آزمون Taber abraser 1000g,H-22Wheel ASTM D1044 4.00 mg Bending modulus 3.20mm ASTM D790 89.6 Mpa
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Linear coefficient of thermal expansion MD ASTM D696 1.5E-04 cm/cm/°C Vicat softening temperature ASTM D15252 80.6 °C Glass transition temperature DSC -15.0 °C
Physical properties شرایط آزمون روش آزمون نتیجه آزمون Shrinkage rate TD ASTM D955 0.60-0.90 % Shrinkage rate MD ASTM D955 0.50-0.90 % melt mass-flow rate 190°C/8.7kg ASTM D1238 13 g/10min
hardness شرایط آزمون روش آزمون نتیجه آزمون Shore hardness ShoreA ASTM D2240 94