TPU 2355-95A LUBRIZOL USA
Pearlthane®
Cable,film,Coating application,Laminate
Flame retardant,Chemical resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | LUBRIZOL USA/2355-95A |
|---|---|---|---|
| Shore hardness | ShoreA | ASTM D2240 | 94 |
| thermal performance | Test Condition | Test Method | LUBRIZOL USA/2355-95A |
|---|---|---|---|
| Glass transition temperature | DSC | -15.0 °C | |
| Linear coefficient of thermal expansion | MD | ASTM D696 | 1.5E-04 cm/cm/°C |
| Vicat softening temperature | ASTM D15252 | 80.6 °C |
| mechanical properties | Test Condition | Test Method | LUBRIZOL USA/2355-95A |
|---|---|---|---|
| Bending modulus | 3.20mm | ASTM D790 | 89.6 Mpa |
| Taber abraser | 1000g,H-22Wheel | ASTM D1044 | 4.00 mg |
| Physical properties | Test Condition | Test Method | LUBRIZOL USA/2355-95A |
|---|---|---|---|
| melt mass-flow rate | 190°C/8.7kg | ASTM D1238 | 13 g/10min |
| Shrinkage rate | MD | ASTM D955 | 0.50-0.90 % |
| TD | ASTM D955 | 0.60-0.90 % |
| elastomer | Test Condition | Test Method | LUBRIZOL USA/2355-95A |
|---|---|---|---|
| elongation | Break,3.20mm | ASTM D412 | 450 % |
| Permanent compression deformation | 70°C,22hr | ASTM D395B | 80 % |
| 25°C,22hr | ASTM D395B | 30 % | |
| tear strength | 3.20mm | ASTM D624 | 105 kN/m |
| tensile strength | 50%Strain,3.20mm | ASTM D412 | 8.30 Mpa |
| 100%Strain,3.20mm | ASTM D412 | 9.70 Mpa | |
| 300%Strain,3.20mm | ASTM D412 | 21.4 Mpa | |
| Break,3.20mm | ASTM D412 | 38.9 Mpa |