برگه داده فنی مقایسهflammability شرایط آزمون روش آزمون نتیجه آزمون UL flame retardant rating 1.5mm UL 94 HB
elastomer شرایط آزمون روش آزمون نتیجه آزمون tensile strength 100%Strain ASTM D412 9.65 Mpa tensile strength 300%Strain ASTM D412 21.4 Mpa tensile strength ASTM D412 35.9 Mpa elongation Break ASTM D412 530 % tear strength ASTM D624 110 kN/m Permanent compression deformation 23°C,22hr ASTM D395B 25 % Permanent compression deformation 70°C,22hr ASTM D395B 45 %
mechanical properties شرایط آزمون روش آزمون نتیجه آزمون Tensile modulus Injection ASTM D412 20.7 Mpa Bending modulus Injection ASTM D790 29.0 Mpa Taber abraser ASTM D1044 30.0 mg Wear resistance DIN 53516 25 mm³
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Glass transition temperature Internal Method -38.0 °C Vicat softening temperature ASTM D1525 100 °C Vicat softening temperature Internal Method 66 °C
Physical properties شرایط آزمون روش آزمون نتیجه آزمون melt mass-flow rate 190°C/21.6kg ASTM D1238 1.0to20 g/10min melt mass-flow rate 190°C/8.7kg ASTM D1238 1.0to10 g/10min
hardness شرایط آزمون روش آزمون نتیجه آزمون Shore hardness ShoreA ASTM D2240 85