برگه داده فنی مقایسهimpact performance شرایط آزمون روش آزمون نتیجه آزمون Charpy Notched Impact Strength 23°C ISO 179/1eA 18 kJ/m² Impact strength of cantilever beam gap 23°C,3.18mm ASTM D256 220 J/m Impact strength of cantilever beam gap 23°C,6.35mm ASTM D256 210 J/m Impact strength of cantilever beam gap 23°C ISO 180/1A 16 kJ/m²
mechanical properties شرایط آزمون روش آزمون نتیجه آزمون bending strength ASTM D790 61.0 Mpa bending strength ISO 178 63.0 Mpa Tensile modulus ASTM D638 2100 Mpa Tensile modulus ISO 527-2/50 2400 Mpa tensile strength Yield ASTM D638 39.0 Mpa tensile strength Yield ISO 527-2/50 42.0 Mpa tensile strength Break ASTM D638 33.0 Mpa tensile strength Break ISO 527-2/50 34.0 Mpa elongation Break ASTM D638 37 % Tensile strain Break ISO 527-2/50 20 % Bending modulus ASTM D790 2200 Mpa Bending modulus ISO 178 2200 Mpa
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Vicat softening temperature ISO 306/B50 94.0 °C Hot deformation temperature 1.8MPa,Unannealed,6.40mm ASTM D648 82.0 °C Hot deformation temperature 1.8MPa,Unannealed,4.00mm ISO 75-2/A 82.0 °C
Physical properties شرایط آزمون روش آزمون نتیجه آزمون density ASTM D792 1.04 g/cm³ density ISO 1183 1.04 g/cm³ melt mass-flow rate 200°C/5.0kg ASTM D1238 3.5 g/10min melt mass-flow rate 200°C/5.0kg ISO 1133 3.5 g/10min Shrinkage rate MD:3.20mm ASTM D955 0.34-0.42 % Shrinkage rate TD:3.20mm ASTM D955 0.36-0.45 % Shrinkage rate TD:3.20mm ISO 2577 0.36-0.45 % Shrinkage rate MD:3.20mm ISO 2577 0.34-0.42 %
hardness شرایط آزمون روش آزمون نتیجه آزمون Rockwell hardness R-Scale ASTM D785 109 Rockwell hardness R-Scale ISO 2039-2 109