برگه داده فنی مقایسهmechanical properties شرایط آزمون روش آزمون نتیجه آزمون Rockwell hardness ISO 2039-2 90 M Impact strength of cantilever beam gap 23℃ ISO 180/1A 5 KJ/m Charpy Notched Impact Strength -30℃ ISO 179/1eA 5 KJ/m Charpy Notched Impact Strength 23℃ ISO 179/1eA 5.5 KJ/m Charpy Notched Impact Strength -30℃ ISO 179/1eU 20 KJ/m Charpy Notched Impact Strength 23℃ ISO 179/1eU 20 KJ/m bending strength 23℃ ISO 178 150 Mpa Bending modulus 23℃ ISO 178 5200 Mpa Elongation at Break 5mm/min ISO 527-2/1A 3.5 % tensile strength 5mm/min ISO 527-2/1A 100 Mpa Tensile modulus 1mm/min ISO 527-2/1A 5800 Mpa
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Melting temperature ISO 11357-1 225 °C Glass transition temperature ISO 11357-1 60 °C Hot deformation temperature 1.8Mpa ISO 75-1/-2 195 °C Hot deformation temperature 0.45Mpa ISO 75-1/-2 215 °C UL flame retardant rating UL 94 HB Extreme Oxygen Index ISO 4589 20 % Hot deformation temperature 8.0Mpa ISO 75-1/-2 90 °C Vicat softening temperature ISO 306 215 °C
Physical properties شرایط آزمون روش آزمون نتیجه آزمون Water absorption rate 23℃,50%相对湿度 ISO 62 0.2 % Water absorption rate 23℃,Saturation ISO 62 0.45 % Shrinkage rate Across Flow ISO 294-4 0.5-0.7 % Melt Volume Flow Rate (MVR) ISO 1133 26 CM
Electrical performance شرایط آزمون روش آزمون نتیجه آزمون Compared to the Leakage Traceability Index (CTI) IEC 60112 350 Dielectric strength IEC 60243-1 29 KV/mm Surface resistivity IEC 60093 >1E15 Ohm Volume resistivity IEC 60093 >1E13 ohm.m Dielectric dissipation factor 1MHz IEC 60250 200 E-4 Dielectric dissipation factor 100Hz IEC 60250 16 E-4 Volume resistivity 1MHz IEC 60250 3.8 Volume resistivity 100Hz IEC 60250 4.2
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.