برگه داده فنی مقایسهOther performance شرایط آزمون روش آزمون نتیجه آزمون Starting temperature of heat sealing Internal Method 85 ℃ Water vapor permeability 38℃,90% RH DIN 53122/2 g·mm/m
Basic Performance شرایط آزمون روش آزمون نتیجه آزمون Monomer content Internal Method %
mechanical properties شرایط آزمون روش آزمون نتیجه آزمون tensile strength Yield,Compression Molded ASTM D-638 7.24 MPa tensile strength Yield,Compression Molded ISO 527-2 7.24 MPa tensile strength Compression Molded,Break ASTM D-638 16.2 MPa tensile strength Compression Molded,Break ISO 527-2 16.2 MPa Elongation at Break Compression Molded ASTM D-638 580 % Elongation at Break Compression Molded ISO 527-2 580 MPa tensile strength Yield,Compression Molded ASTMD638 7.24 Mpa tensile strength Break,Compression Molded ASTMD638 16.2 Mpa elongation Break,Compression Molded ASTMD638 580 %
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Vicat softening temperature ASTM D-1525 72.2 ℃ Vicat softening temperature ISO 306 72.2 ℃ Melting temperature Internal Method ℃ Vicat softening temperature ASTMD1525 72.2 °C Melting temperature Internal Method 95.0 °C
Physical properties شرایط آزمون روش آزمون نتیجه آزمون melt mass-flow rate 190°C/2.16kg ASTMD1238 20 g/10min Content of comonomer Internal Method 9.7 %
film شرایط آزمون روش آزمون نتیجه آزمون Initial sealing temperature Internal Method 85.0 °C Water vapor permeability 38°C,90%RH DIN 53122/2 0.44 g·mm/m²/atm/24hr