برگه داده فنی مقایسهelastomer شرایط آزمون روش آزمون نتیجه آزمون Permanent compression deformation 70°C,22hr ASTMD395 46 % Permanent compression deformation 23°C,22hr ASTMD395 24 % tear strength 0.635mm DIN 53515 45 kN/m tear strength 0.635mm ASTM D624 89.3 kN/m elongation Break,0.635mm DIN 53504 750 % elongation Break,0.635mm ASTM D412 810 % tensile strength Break,0.635mm DIN 53504 30.0 Mpa tensile strength Break,0.635mm ASTM D412 21.0 Mpa tensile strength 300%Strain,0.635mm DIN 53504 8.40 Mpa tensile strength 300%Strain,0.635mm ASTM D412 8.27 Mpa tensile strength 100%Strain,0.635mm DIN 53504 5.70 Mpa tensile strength 100%Strain,0.635mm ASTM D412 5.93 Mpa
mechanical properties شرایط آزمون روش آزمون نتیجه آزمون Wear resistance -- 54 mm³ Wear resistance -- DIN 53515 50 mm³
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Melting temperature TMA 126to150 °C
Physical properties شرایط آزمون روش آزمون نتیجه آزمون Shrinkage rate MD:Injection ASTM D955 11 % Melt Volume Flow Rate (MVR) 190°C/21.6kg 140 cm3/10min
hardness شرایط آزمون روش آزمون نتیجه آزمون Shore hardness ShoreA,Injection ASTMD2240 81
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.