برگه داده فنی مقایسهelastomer شرایط آزمون روش آزمون نتیجه آزمون tensile strength 100%Strain ASTM D412 8.96 Mpa tensile strength 100%Strain DIN 53504 9.10 Mpa tensile strength 300%Strain ASTM D412 14.1 Mpa tensile strength 300%Strain DIN 53504 15.9 Mpa tensile strength Break ASTM D412 33.6 Mpa tensile strength Break DIN 53504 45.0 Mpa elongation Break ASTM D412 670 % elongation Break DIN 53504 600 % tear strength ASTM D624 116 kN/m tear strength ISO 34-1 74 kN/m Permanent compression deformation 23°C,24hr ASTM D395 25 % Permanent compression deformation 70°C,24hr ASTM D395 41 % Permanent compression deformation 23°C,24hr ISO 815 25 % Permanent compression deformation 70°C,24hr ISO 815 41 % Permanent compression deformation 巴肖氏弹性 ISO 815 34 %
mechanical properties شرایط آزمون روش آزمون نتیجه آزمون Wear resistance ISO 4649 30 mm³
Physical properties شرایط آزمون روش آزمون نتیجه آزمون Melt Volume Flow Rate (MVR) 190°C/21.6kg 55.0 cm3/10min Shrinkage rate MD ASTM D955 0.40 % Shrinkage rate 0.90 %
hardness شرایط آزمون روش آزمون نتیجه آزمون Shore hardness ShoreA,Injection ASTM D2240 92 Shore hardness ShoreD,Injection ASTM D2240 39 Shore hardness ShoreA,Injection ISO 868 92 Shore hardness ShoreD,Injection ISO 868 39
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.