TPU A92P4637 HUNTSMAN GERMANY
IROGRAN®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | HUNTSMAN GERMANY/A92P4637 |
---|---|---|---|
邵氏A,注塑 | ASTMD2240 | 92 | |
邵氏A,注塑 | ISO868 | 92 | |
邵氏D,注塑 | ISO868 | 39 | |
邵氏D,注塑 | ASTMD2240 | 39 |
Mechanical properties | Test Condition | Test Method | HUNTSMAN GERMANY/A92P4637 |
---|---|---|---|
Abrasion2 | ISO4649 | 30 mm³ |
physical property | Test Condition | Test Method | HUNTSMAN GERMANY/A92P4637 |
---|---|---|---|
Melt volume flow rate | 190°C/21.6kg | 55.0 cm3/10min | |
Shrinkage rate | MD | ASTMD955 | 0.40 % |
0.90 % |
elastomer | Test Condition | Test Method | HUNTSMAN GERMANY/A92P4637 |
---|---|---|---|
elongation | 断裂 | ASTMD412 | 670 % |
Compression permanent deformation 2 | 23°C,24hr | ASTMD395 | 25 % |
Tear strength 2 | ASTMD624 | 116 kN/m | |
Compression permanent deformation 2 | 巴肖氏弹性 | ISO815 | 34 % |
70°C,24hr | ISO815 | 41 % | |
Tensile stress 2 | 100%应变 | DIN53504 | 9.10 Mpa |
300%应变 | ASTMD412 | 14.1 Mpa | |
elongation | 断裂 | DIN53504 | 600 % |
Tensile stress 2 | 300%应变 | DIN53504 | 15.9 Mpa |
Compression permanent deformation 2 | 23°C,24hr | ISO815 | 25 % |
Tear strength 2 | ISO34-1 | 74 kN/m | |
Tensile stress 2 | 100%应变 | ASTMD412 | 8.96 Mpa |
tensile strength | 断裂 | ASTMD412 | 33.6 Mpa |
Compression permanent deformation 2 | 70°C,24hr | ASTMD395 | 41 % |
Tensile stress 2 | 断裂 | DIN53504 | 45.0 Mpa |