برگه داده فنی مقایسهmechanical properties شرایط آزمون روش آزمون نتیجه آزمون bending strength 23°C ISO 178 230 Mpa Friction coefficient Dynamic2 ASTM D1894 0.28 Friction coefficient Dynamic3 ASTM D1894 0.28 Friction coefficient Static2 ASTM D1894 0.29 Friction coefficient Static3 ASTM D1894 0.30 Friction coefficient Steel - Dynamic4 ASTM D1894 0.15 Friction coefficient Steel - Static4 ASTM D1894 0.17 Wear factor 416Stainless:32°C ASTM D3702 148 10^-10in³·min/ft·lb·hr Wear factor C-1018Steel:49°C ASTM D3702 120 10^-10in³·min/ft·lb·hr Wear factor C-1018Steel:93°C ASTM D3702 415 10^-10in³·min/ft·lb·hr tensile strength Break ISO 527-2/1A/5 150 Mpa Tensile strain Break ISO 527-2/1A/5 1.9 % Bending modulus 23°C ISO 178 10600 Mpa
thermal performance شرایط آزمون روش آزمون نتیجه آزمون Hot deformation temperature 1.8MPa,Unannealed ISO 75-2/A 260 °C Hot deformation temperature 8.0MPa,Unannealed ISO 75-2/C 190 °C
Physical properties شرایط آزمون روش آزمون نتیجه آزمون Shrinkage rate TD ISO 294-4 0.60-0.90 % Shrinkage rate MD ISO 294-4 0.30-0.50 % Water absorption rate Equilibrium,23°C,50%RH ISO 62 0.020 %
نکات مهم: Plas.com دادههای برگه فنی را از تولیدکنندگان مواد جمعآوری کرده است. Plas.com تمام تلاش خود را برای افزایش دقت دادهها انجام میدهد، اما هیچ مسئولیتی در قبال دادهها ندارد. اکیداً توصیه میشود که صحت دادهها را با تولیدکنندگان مواد تأیید کنید پیش از آنکه تصمیم نهایی بگیرید.