物性数据
| 光学性能 | 测试条件 | 测试方法 | 测试结果 |
|---|
| 表观密度 | 10.0µm | Internal Method | -2.8-7.2 % |
| 表观密度 | 12.0µm | Internal Method | -2.8-7.2 % |
| 表观密度 | 23.0µm | Internal Method | -2.8-7.2 % |
| 表观密度 | 36.0µm | Internal Method | -2.8-7.2 % |
| 表观密度 | 50.0µm | Internal Method | -2.8-7.2 % |
| 物理性能 | 测试条件 | 测试方法 | 测试结果 |
|---|
| 收缩率 | MD:150°C,30分钟,0.0500mm | ASTM D1204 | 2.5 % |
| 收缩率 | TD:150°C,30分钟,0.0100mm | ASTM D1204 | 0.40 % |
| 收缩率 | TD:150°C,30分钟,0.0120mm | ASTM D1204 | 0.40 % |
| 收缩率 | TD:150°C,30分钟,0.0230mm | ASTM D1204 | 0.40 % |
| 收缩率 | TD:150°C,30分钟,0.0360mm | ASTM D1204 | 0.40 % |
| 收缩率 | TD:150°C,30分钟,0.0500mm | ASTM D1204 | 0.40 % |
| 表面强度 | 10.0µm,金属化面 | ASTM D2578 | 56 mN/m |
| 表面强度 | 12.0µm,金属化面 | ASTM D2578 | 56 mN/m |
| 表面强度 | 23.0µm,金属化面 | ASTM D2578 | 56 mN/m |
| 表面强度 | 36.0µm,金属化面 | ASTM D2578 | 56 mN/m |
| 表面强度 | 50.0µm,金属化面 | ASTM D2578 | 56 mN/m |
| 收缩率 | MD:150°C,30分钟,0.0100mm | ASTM D1204 | 2.5 % |
| 收缩率 | MD:150°C,30分钟,0.0120mm | ASTM D1204 | 2.5 % |
| 收缩率 | MD:150°C,30分钟,0.0230mm | ASTM D1204 | 2.5 % |
| 收缩率 | MD:150°C,30分钟,0.0360mm | ASTM D1204 | 2.5 % |
| 薄膜 | 测试条件 | 测试方法 | 测试结果 |
|---|
| 用量 | 50.0µm | Internal Method | 14.3 m²/kg |
| 薄膜厚度 | | | 10122336 µm |
| 薄膜厚度 | | | 10.12.23.36.50µm |
| 拉伸强度 | MD:断裂,10µm | ASTM D882 | 206 MPa |
| 拉伸强度 | MD:断裂,12µm | ASTM D882 | 206 MPa |
| 拉伸强度 | MD:断裂,23µm | ASTM D882 | 186 MPa |
| 拉伸强度 | MD:断裂,36µm | ASTM D882 | 177 MPa |
| 拉伸强度 | MD:断裂,50µm | ASTM D882 | 167 MPa |
| 拉伸强度 | TD:断裂,10µm | ASTM D882 | 216 MPa |
| 拉伸强度 | TD:断裂,12µm | ASTM D882 | 216 MPa |
| 伸长率 | TD:断裂,23µm | ASTM D882 | 90 % |
| 伸长率 | TD:断裂,36µm | ASTM D882 | 120 % |
| 伸长率 | TD:断裂,50µm | ASTM D882 | 120 % |
| 氧气透过率 | 23°C,10µm | ASTM D3985 | 0.900 cm³/m²/24hr |
| 氧气透过率 | 23°C,12µm | ASTM D3985 | 0.900 cm³/m²/24hr |
| 氧气透过率 | 23°C,23µm | ASTM D3985 | 0.800 cm³/m²/24hr |
| 氧气透过率 | 23°C,36µm | ASTM D3985 | 0.800 cm³/m²/24hr |
| 氧气透过率 | 23°C,50µm | ASTM D3985 | 0.800 cm³/m²/24hr |
| 水蒸气透过率 | --2 | ASTMF1249 | 0.60 g/m²/24hr |
| 水蒸气透过率 | --3 | ASTMF1249 | 0.60 g/m²/24hr |
| 水蒸气透过率 | --4 | ASTMF1249 | 0.60 g/m²/24hr |
| 拉伸强度 | TD:断裂,23µm | ASTM D882 | 206 MPa |
| 拉伸强度 | TD:断裂,36µm | ASTM D882 | 186 MPa |
| 拉伸强度 | TD:断裂,50µm | ASTM D882 | 186 MPa |
| 伸长率 | MD:断裂,10µm | ASTM D882 | 100 % |
| 伸长率 | MD:断裂,12µm | ASTM D882 | 100 % |
| 伸长率 | MD:断裂,23µm | ASTM D882 | 100 % |
| 伸长率 | MD:断裂,36µm | ASTM D882 | 130 % |
| 伸长率 | MD:断裂,50µm | ASTM D882 | 130 % |
| 伸长率 | TD:断裂,10µm | ASTM D882 | 90 % |
| 伸长率 | TD:断裂,12µm | ASTM D882 | 90 % |
| 水蒸气透过率 | --5 | ASTMF1249 | 0.60 g/m²/24hr |
| 水蒸气透过率 | --6 | ASTMF1249 | 0.60 g/m²/24hr |
| 用量 | 10.0µm | Internal Method | 71.4 m²/kg |
| 用量 | 12.0µm | Internal Method | 59.5 m²/kg |
| 用量 | 23.0µm | Internal Method | 31.0 m²/kg |
| 用量 | 36.0µm | Internal Method | 19.8 m²/kg |
免责声明:此数据表中的信息由 Plas.Com 从该材料的生产商或第三方处获得。Plas.Com 尽最大努力确保此数据的准确性。 但是 Plas.Com 对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。