原料比对

产品信息
品名
品牌名
典型应用
特性
认证
MVLDPE 1018EA EXXONMOBIL USA
Exceed™ 
film、Bag、Lining、chip
high strength、High impact resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

物性数据

Films Properties测试条件测试方法EXXONMOBIL USA/1018EA
Elongation - MD断裂ASTMD882500 %
Elmendorf Tear Strength (MD)ASTMD1922250 g
Gardner ImpactASTMD1709A460 g
Secant Modulus (1%Secant,TD)ASTMD882192 Mpa
Tensile Strength (TD)YieldASTMD8829.40 Mpa
Elmendorf Tear Strength (TD)ASTMD1922470 g
Tensile Strength-MD断裂ASTMD88254.3 Mpa
Secant Modulus (1%Secant,MD)ASTMD882185 Mpa
Tensile Strength-MD屈服ASTMD8829.37 Mpa
Tensile Strain (TD)BreakASTMD882600 %
Tensile Strength (TD)断裂ASTMD88242.7 Mpa
Physical测试条件测试方法EXXONMOBIL USA/1018EA
Melt Mass-Flow Rate190°C/2.16kgASTMD12381.0 g/10min
Optical测试条件测试方法EXXONMOBIL USA/1018EA
HazeASTMD100318 %
Gloss45°ASTMD245739