1,000 products

Manufacturer: Nizhnekamskneftekhim Inc.
Clear all filters
MaterialsMaterial DescriptionCertificatesReference PriceOperate
ABS Nizhnekamskneftekhim Inc. NEFTEKHIM ABS 1035
Impact strength of cantilever beam gap 10 melt mass-flow rate 8.5to12 Hot deformation temperature 103 tensile strength 40.0
-- --
HDPE Nizhnekamskneftekhim Inc. NEFTEKHIM PE 6844G (446H7)
melt mass-flow rate 0.60to0.80 density 0.942to0.946 Bending modulus 900 Impact strength of cantilever beam gap 300
-- --
LLDPE Nizhnekamskneftekhim Inc. NEFTEKHIM PE 4118P (18402)
melt mass-flow rate <30.0 density 0.916to0.920 tensile strength 24.0
-- --
PP Nizhnekamskneftekhim Inc. NEFTEKHIM PP 8540N (EPF31H)
melt mass-flow rate 10to15 Impact strength of cantilever beam gap 30 Bending modulus 1350
-- --
PP Nizhnekamskneftekhim Inc. NEFTEKHIM PP 5254M (RCXP925)
melt mass-flow rate 9.0to12 Bending modulus 950 tensile strength 27.0
-- --
PP Nizhnekamskneftekhim Inc. NEFTEKHIM PP 4240G (EP2S29B)
melt mass-flow rate 1.5to2.0 Impact strength of cantilever beam gap 90 Bending modulus 950 tensile strength 27.0
-- --
PP Copolymer Nizhnekamskneftekhim Inc. NEFTEKHIM PP 8332C (EPD60R)
melt mass-flow rate 0.50to0.90 Impact strength of cantilever beam gap 60
-- --
PP Nizhnekamskneftekhim Inc. NEFTEKHIM PP 8340K
melt mass-flow rate 3.5to4.5 Impact strength of cantilever beam gap 50 Bending modulus 1100
-- --
PP Homopolymer Nizhnekamskneftekhim Inc. NEFTEKHIM PP 1501M
melt mass-flow rate 7.0to10 Impact strength of cantilever beam gap 30 tensile strength 33.0
-- --
MDPE Nizhnekamskneftekhim Inc. NEFTEKHIM PE 4440R (40404)
melt mass-flow rate 3.5to4.5 Impact strength of cantilever beam gap 无断裂
-- --
PP Homopolymer Nizhnekamskneftekhim Inc. NEFTEKHIM PP 1500J (T30G)
melt mass-flow rate 2.4to3.7 Impact strength of cantilever beam gap 45 tensile strength 34.0
-- --
ABS Nizhnekamskneftekhim Inc. NEFTEKHIM ABS 2332
Impact strength of cantilever beam gap 11 melt mass-flow rate 20to26 Hot deformation temperature 96 tensile strength 45.0
-- --
PP Homopolymer Nizhnekamskneftekhim Inc. NEFTEKHIM PP PP6129K
melt mass-flow rate 5.0 Impact strength of cantilever beam gap 60 tensile strength 20.0
-- --
PP Nizhnekamskneftekhim Inc. NEFTEKHIM PP 1554N (F79S)
melt mass-flow rate 10to14 Bending modulus 1400 tensile strength 33.0
-- --
PP Nizhnekamskneftekhim Inc. NEFTEKHIM PP 5215M (RCXP722)
melt mass-flow rate 9.0to12 Bending modulus 950 tensile strength 27.0
-- --
PP Nizhnekamskneftekhim Inc. NEFTEKHIM PP 2641J (T31SE)
melt mass-flow rate 3.3to4.2 Impact strength of cantilever beam gap 40 Bending modulus 1500 tensile strength 34.0
-- --
PP Homopolymer Nizhnekamskneftekhim Inc. NEFTEKHIM PP 1551J (T30SW)
melt mass-flow rate 2.9to3.5 tensile strength 34.0
-- --
PP Nizhnekamskneftekhim Inc. NEFTEKHIM PP 1462R (HOXP817)
melt mass-flow rate 20to30 Bending modulus 1300
-- --
PP Nizhnekamskneftekhim Inc. NEFTEKHIM PP 4348S
melt mass-flow rate 35to45 Impact strength of cantilever beam gap 45 Bending modulus 950
-- --
HDPE Nizhnekamskneftekhim Inc. NEFTEKHIM PE 6433R (32604)
melt mass-flow rate 3.5to4.5 density 0.930to0.934 Bending modulus 620 Impact strength of cantilever beam gap 无断裂
-- --