Rubber LinGen HT175

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D7920.950 g/cm³
hardnessTest ConditionTest MethodTest Result
Hardness (Shore)Shore AASTM D224075
elastomerTest ConditionTest MethodTest Result
tensile strength YieldASTM D41211.0 MPa
elongationBreakASTM D412600 %
tear strengthASTM D62430.0 kN/m
compression setASTM D39519 %
compression setASTM D39530 %
Thermal performanceTest ConditionTest MethodTest Result
brittle temperatureASTM D746-60.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.