TPE 1165
0
- Properties:Injection molding reference process feeding section temperature150-160 ℃model temperature10-50 ℃middle section temperature170-190 ℃screw speed100-200rminfront section temperature180-220 ℃back pressure01-10MPanozzle temperature180-230 ℃injection pressuremedium high MPaextrusion reference process barrel feeding section temperature 130-150?
Technical Data Sheet
Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
relative density | 0.96 g/cm |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Elongation | 740 % | ||
stretching strength | 1.6 MPa | ||
Shore hardness | 65 A | ||
tensile strength | 8.0 MPa | ||
tear strength | 25.0 kN/m |
Other performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile strength retention rate | 106 % | ||
compression set | 25 | ||
Retention rate of elongation at break | 95 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.