Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTMD1505 | 0.923 g/cm³ | |
melt mass-flow rate | ASTMD1238 | 2.0 g/10min |
optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
gloss | ASTMD2457 | 75 | |
Haze ratio | ASTMD1003 | 5.0 % |
film | Test Condition | Test Method | Test Result |
---|---|---|---|
Elmondov tear strength MD | ASTMD1922 | 350 g | |
ElmendorfTearStrength-TD | ASTMD1922 | 180 g | |
Secant modulus | ASTMD882 | 214 MPa | |
ASTMD882 | 255 MPa | ||
tensile strength | Yield | ASTMD882 | 24.8 MPa |
tensile strength | ASTMD882 | 21.4 MPa | |
elongation | Break | ASTMD882 | 200 % |
Tensile strain | ASTMD882 | 600 % | |
Falling hammer impact | ASTMD1709 | 100 g |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.