THV Dyneon™  815GZ

27

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
melt mass-flow rateISO113315 g/10min
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile stressISO527-229.0 Mpa
Tensile strainISO527-2430 %
Flexural modulusASTMD790525 Mpa
Thermal performanceTest ConditionTest MethodTest Result
melting temperatureISO12086225 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.