Technical Data Sheet
物理性能 | Test Condition | Test Method | Test Result |
---|
密度 | | ASTMD792 | 1.32 g/cm³ |
收缩率 | MD:3.00mm | ASTMD955 | 2.0 % |
吸水率 | 24hr | ASTMD570 | 0.060 % |
机械性能 | Test Condition | Test Method | Test Result |
---|
弯曲模量 | | ASTMD790 | 3000 MPa |
弯曲强度 | Yield | ASTMD790 | 98.0 MPa |
抗张强度 | Yield | ASTMD638 | 56.0 MPa |
伸长率 | Break | ASTMD638 | 100 % |
可燃性 | Test Condition | Test Method | Test Result |
---|
UL阻燃等级 | | UL94 | HB |
电气性能 | Test Condition | Test Method | Test Result |
---|
体积电阻率 | | ASTMD257 | 1E+17 ohms·cm |
介电强度 | 2.00mm | ASTMD149 | 24 kV/mm |
耐电弧性 | | ASTMD495 | 130 sec |
硬度 | Test Condition | Test Method | Test Result |
---|
洛氏硬度 | M-Scale | ASTMD785 | 80 |
热性能 | Test Condition | Test Method | Test Result |
---|
热变形温度 | 1.8MPa,未退火 | ASTMD648 | 65.0 °C |
线性热膨胀系数 | MD | ASTMD696 | 8E-05 cm/cm/°C |
悬壁梁缺口冲击强度 | | ASTMD256 | 45 J/m |
热变形温度 | 0.45MPa,未退火 | ASTMD648 | 165 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.