PC LEV1700 IDEMITSU JAPAN
110
Form:Granules | Grade:Injection grade
Properties:
heat-resisting
Typical Applications:
Automotive Applications
Product Description
Certificates(0)
Datasheet
Product Description
| Typical Applications: | Automotive Applications |
| Properties: | heat-resisting |
Certificates
No Data...
Technical Data Sheet
| optical performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Refractive index | ASTM D542 | 1.585 | ||
| transmissivity | ISO 13468-1 | 90.0 | % | |
| flammability | Test Condition | Test Method | Test Result | Test Unit |
| UL flame retardant rating | 0.40mm | UL 94 | V-2 | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | Yield | ISO 527-2 | 65 | Mpa |
| Elongation at Break | ISO 527-2 | 95 | % | |
| Bending modulus | ISO 178 | 2300 | Mpa | |
| bending strength | ISO 178 | 90 | Mpa | |
| Charpy Notched Impact Strength | ISO 179 | 40 | kJ/m² | |
| tensile strength | Yield | ISO 527-2 | 65.0 | Mpa |
| Nominal tensile fracture strain | ISO 527-2 | 95 | % | |
| Bending modulus | ISO 178 | 2300 | Mpa | |
| bending strength | ISO 178 | 90.0 | Mpa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8 MPa, Unannealed | ISO 75-2/A | 128 | °C |
| Linear coefficient of thermal expansion | ISO 11359-2 | 0.000065 | cm/cm/℃ | |
| UL flame retardant rating | 0.400 mm | UL 94 | V-2 | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 129 | °C |
| Linear coefficient of thermal expansion | MD | ISO 11359-2 | 6.5E-05 | cm/cm/°C |
| RTI Elec | UL 746 | 80.0 | °C | |
| RTI Imp | UL 746 | 80.0 | °C | |
| RTI Str | UL 746 | 80.0 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Melt Volume Flow Rate (MVR) | MVR | ISO 1133 | 40 | cm3/10min |
| Shrinkage rate | TD | Internal Method | 0.5-0.7 | % |
| MD: 2.00 mm | Internal Method | 0.5-0.7 | % | |
| Water absorption rate | Equilibrium,23℃, 50% RH | ISO 62 | 0.23 | % |
| Melt Volume Flow Rate (MVR) | 300°C/1.2kg | ISO 1133 | 27.0 | cm3/10min |
| Shrinkage rate | TD:2.00mm | Internal Method | 0.50-0.70 | % |
| MD:2.00mm | Internal Method | 0.50-0.70 | % | |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.23 | % |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Rockwell hardness | M-Sale | ISO 2039-2 | 50 | |
| R-Sale | ISO 2039-2 | 120 | ||
| Supplementary Information | Test Condition | Test Method | Test Result | Test Unit |
| ISO Shortcut | >PC< |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.