Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Water absorption rate | | ISO 62 | 2.4 % |
Shrinkage rate | | ISO 294-4 | 1.5 % |
Shrinkage rate | | ISO 294-4 | 1.5 % |
density | | ISO 1183 | 1.43 g/cm³ |
flammability | Test Condition | Test Method | Test Result |
---|
Flammability level | | UL 94 | V-0 |
Flammability level | | UL 94 | V-0 |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Charpy Notched Impact Strength | | ISO 179/1eA | 4.0 kJ/m² |
Charpy Notched Impact Strength | | ISO 179/1eA | 3.0 kJ/m² |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Flexural modulus | | ISO 178 | 3200 Mpa |
Nominal tensile fracture strain | | ISO 527-2 | 7.0 % |
tensile strength | | ISO 527-2 | 80.0 Mpa |
Tensile modulus | | ISO 527-2 | 3400 Mpa |
Electrical performance | Test Condition | Test Method | Test Result |
---|
relative permittivity | | IEC 60250 | 3.50 |
relative permittivity | | IEC 60250 | 3.80 |
dielectric strength | | IEC 60243-1 | 30 KV/mm |
Volume resistivity | | IEC 60093 | 1.0E+15 ohms·cm |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Linear coefficient of thermal expansion | | ISO 11359-2 | 9.0E-5 cm/cm/°C |
Linear coefficient of thermal expansion | | ISO 11359-2 | 8.0E-5 cm/cm/°C |
melting temperature | | ISO 11357-3 | 295 °C |
Heat distortion temperature | | ISO 75-2/A | 190 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.