Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ISO 1183/A | 1.43 g/cm³ |
Dissolved volume flow rate | | ISO 1133 | 18.0 cm³/10min |
other | Test Condition | Test Method | Test Result |
---|
Flammability level | | IEC 60695-11-10, -20 | HB |
Flammability level | | IEC 60695-11-10, -20 | HB |
Burning wire flammability index | | IEC 60695-2-12 | 700 ℃ |
Hot filament ignition temperature | | IEC 60695-2-13 | 725 ℃ |
Hot filament ignition temperature | | IEC 60695-2-13 | 775 ℃ |
Limiting Oxygen Index | | ISO 4589-2 | 20 % |
flammability | | FMVSS 302 | 30 mm/min |
Burning wire flammability index | | IEC 60695-2-12 | 750 ℃ |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Charpy Notched Impact Strength | | ISO 179/1eU | 40 kJ/m² |
Tensile modulus | | ISO 527-2/1A/1 | 10000 MPa |
Tensile stress | Break | ISO 527-2/1A/5 | 125 MPa |
Tensile strain | Break | ISO 527-2/1A/5 | 2.0 % |
Flexural modulus | | ISO 178 | 8500 MPa |
bending strength | | ISO 178 | 172 MPa |
Charpy Notched Impact Strength | | ISO 179/1eA | 7.0 kJ/m² |
Charpy Notched Impact Strength | | ISO 179/1eA | 7.0 kJ/m² |
Charpy Notched Impact Strength | | ISO 179/1eU | 35 kJ/m² |
Electrical performance | Test Condition | Test Method | Test Result |
---|
CTI | | IEC 60112 | 200 V |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ISO 75-2/Bf | 213 ℃ |
| | ISO 75-2/Af | 186 ℃ |
vicat | | ISO 306/A50 | 202 ℃ |
vicat | | ISO 306/B50 | 133 ℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.