| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179 | 6.0 | kJ/m² | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| Tensile strain | Break | ISO 527-2 | 20 | % |
| Tensile modulus | ISO 527-2 | 2500 | MPa | |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | VicatB | ISO 306 | 82 | °C |
| thermal conductivity | DIN 52612 | 0.16 | W/m/K | |
| Linear coefficient of thermal expansion | MD | DIN 53752 | 6.0E-5到8.0E-5 | cm/cm/°C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | <3.0 | % |
| density | ISO 1183 | 1.40 | g/cm³ | |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Surface resistivity | IEC 60093 | >1.0E+13 | ohms | |
| Dissipation factor | 1MHz | IEC 60250 | 0.020 | |
| Dielectric constant | IEC 60250 | 3.20 | ||
| Volume resistivity | IEC 60093 | >1.0E+15 | ohms·cm | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreD | ISO 868 | 80 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.